mauricethegangsteroflove - 17-3-2026 at 16:05

I found myself in need of a source of vacuum to use with a filtration flask I recently acquired, and lacking a suitable pump I 3D printed an adapter to connect the hose from the flask to my vacuum cleaner. I hadn't really considered printing lab equipment or supplies before but the adapter worked well enough, and now I'm thinking of possibilities for custom test tube racks, clamps, etc.

What kinds of things have you printed, or would like to try printing? Nylon filament can be quite heat resistant, and PLA is probably suitable for many low temp or disposable purposes. Perhaps keck clips could be printable. I'm curious what others have tried, and to hear any success or failure stories.

Twospoons - 17-3-2026 at 17:37

I don't have a lab jack, so I printed some stackable tripod legs so I could raise my heating mantle off the bench.

chempyre235 - 18-3-2026 at 07:40

I've done some printing with PLA, and it works well enough for most things. I haven't tried it with lab equipment though. There are a few threads on this subject:
https://www.sciencemadness.org/whisper/viewthread.php?tid=24...
https://www.sciencemadness.org/whisper/viewthread.php?tid=96...
https://www.sciencemadness.org/talk/viewthread.php?tid=15553...
I seem to remember someone printing some beakers and such, but I can't find the thread.

I've also tried ABS, which is more chemical/temperature resistant, but I think I need an enclosure to keep the up the temp while printing. ABS is notorious for requiring high heat, and doesn't self-bond as well as PLA. Nearly every ABS print I've tried has looked like a Christmas tree, because the layers didn't stick together well enough, and also didn't cool evenly.

[Edit]: @Twospoons, I don't think printing a simple lab jack would be that hard. It's just a scissor table with a long screw for adjustment. Could be fun to try.

[Edited on 3/18/2026 by chempyre235]

Deathunter88 - 18-3-2026 at 09:44

Consumer 3D printing has come a long way in the last 5 years or so. Before your main choices was PLA, ABS, PETG and at the time even ASA was a new development.

Now we can print:

PPS and PPS-CF, which is almost as chemically resistant as Teflon.

We have PPA-CF which is almost as strong as 6063 aluminum.

PEBA which I think of as 3D printable Viton-like rubber (it's almost as chemically resistant with a few exceptions).

All of these can easily be printed by the Elegoo Centauri Carbon, a $300 printer. It's frankly amazing what you can do with consumer 3D printing nowadays.

For example, I recently printed a nitric acid digester using PPS-CF, and it withstood concentrated HNO3 at 120C.

semiconductive - 18-3-2026 at 11:00

I have an elegoo Saturn. I've printed test tube fixtures with it in the past.

I plan on using ground glass dust and the UV curable (thermoset) resin to print a refractometer within a month. It makes high precision parts.

I just purchased a $350 rock tumbler barrel that is stainless steel to do ball milling of glass with. eg: The optical cure resins don't melt, and become extra strong with glass dust as filler.

chempyre235 - 18-3-2026 at 11:26

Aha! I found it. @Arkoma printed the beakers.

I've got an Ender 3-v2 printer with some upgrades that I bought, like a titanium heating chamber. I haven't put the printer to much use for the last few years, though. I've mostly done PLA, but I don't seem to have the necessary equipment for high-temp ABS or PPS.

violet sin - 18-3-2026 at 14:11

Elegoo centauri carbon

I was on a hot streak yesterday, had that thing running 21hrs almost straight for a 6th grade life skills class, my son was learning economics at a school function. We did a mess of dummy-13 (PLA /PETG), some articulated dragons/mini-dragons (PLA). So I've been getting more familiar with orca slicer, trying to find time to get into blender too. I'm slowly getting the hang of adding supports, brims, adjusting scale and size. Taking notes as I go so the filaments get easier.

I've only printed a few useful things like, light switch/outlet covers before a renewal on our leas walk through. Hoping it will be another boost in capabilities as opposed to a time gobbling entropy well.

The thing came with a couple reels of PLA-CF so that was nice. Found some reg PLA, PETG, and silk I think at the "bin store" remainder/return lot seller. A stack of build plates for 1$/EA that are for the X1C. Just a couple mm off from my stock build plate, and they leave either carbon fiber look or shattered diamond look to the bottom of your pieces, kinda cool.

If I get back into chem hobby at the practicing level, I'd definitely consider printing stuff

IMG_20260311_151016821.jpg - 2.8MB

Elegoo CC is single color, so this was hand fed in chunks for artistic fun. Definitely don't suggest standing there for an hour on every print, but in this case it was nice to see what I could do without having automatic color changes.

Hope y'all have a great day
-VS

IMG_20260316_175539568_HDR.jpg - 2.8MB

SnailsAttack - 21-3-2026 at 04:06

It's funny that you made this post, because just this month I finally gained access to my school's 3D printer (uses PLA) and figured out how to use a CAD modeling software (OnShape) specifically to produce custom labware.

I was able to print some early prototypes this thursday. This first one is a highly modular rack for my smaller test tubes. It was too specific to purchase and too hard to make out of popsicle sticks, the perfect candidate for a CAD solution.

IMG_0450.jpg - 470kB IMG_0451.jpg - 288kB

Modular approach will let me mix and match parts and easily produce new ones.

Besides this, I also designed another rack to organize the medicine bottles I use to store all my chemicals.

IMG_0261.jpeg - 592kB IMG_0262.jpeg - 444kB

Untitled.png - 197kB IMG_0263.jpeg - 792kB

Was this an unreasonable investment of time and effort just so my chemicals wouldn't have to be stored rolling around in a box? Yes. Nonetheless, I think this will be a great return on investment, because I am finally, FINALLY absolved of having to make these god damn arts and crafts cardboard boxes.

As with the test tube rack, the bottle rack is modular. The current 1x3 model is designed so that multiple copies can be coupled by inserting the two smaller pins. The connection is sturdy enough to lift an entire array of filled bottles.

These projects were both fairly trivial (literally the only design constraint was that the parts fit together and aren't too easy to accidentally snap in half), but demonstrate that I now have the means to synthesize complex and highly specific items like tools, adapters and fittings, etc.