SupaVillain - 22-11-2015 at 15:25
Looking again for more materials inert with these chems below, does polyvinylchloride(PVC) react with them? Ordinary rubber stoppers from
lowes/homedepot? These prismacolor magic rub erasers take an insulin syringe needle very well, they are "PVC, abrasive, plasticizer (6422-86-2,
120-55-8)" will they work? (MSDS: http://msdsdigital.com/prismacolor-magic-rub-eraser-msds)
Disilane
dimethylzinc
phosphine
triphenylarsine
trimethylaluminum
trimethylgallium
trimethylindium
Germanium Ethoxide
I have prepared arduino uno with MG996R high torque servos to move syringes around like a cnc machine and run the MOVPE processes through substrate
holder in an inert atmosphere glove box except with me hopefully monitoring from far away. Those magic rub erasers have a lower risk of bending the 31
gauge needles and would prevent any need for extra maintenance.