What is the composition of mouse/insects trape glue? what is the type of this glue?

not_important - 23-10-2006 at 01:19

Often a low grade of rubber, occasionally a synthetic rubber, and mineral oil or similar high boiling hydrocarbon to function as a solvent to keep the rubber soft.

bio2 - 23-10-2006 at 09:32

One I have says polyisobutylene and this stuff is the stickiest
shit I've ever seen.