SAM4CH - 16-12-2006 at 02:21
I need help in design my perchlorate cell!! I get very good results which I can make 2600g per 4days at 120A and 6Volts with no buffer or HCl added! I
faced many problems in my 6Liter cell like connection and install the lead dioxide anodes "I past it with fiber and epoxy glue but I faced problem
when I like to reinstall new anode if one of them has crack, my anodes number is four and 12mm, 30,5cm Gouging rods coated with 4-5mm PbO2" I need
mechanical and chemical help because in last week my cell explode after 10minutes of operation and I think that cause of hydrogen gas but I let
Hydrogen to escape through 20mm hole, and my cell provided with Exhaust Fans..
my current cell has these dimensions :
5cm width * 25 hight *50 long cm the case is stainless steel 304 and it is cathode (-)
FrankRizzo - 14-1-2007 at 13:23
Would you mind posting photos of your setup? Also, what are you using for such a high current power supply?
[Edited on 14-1-2007 by FrankRizzo]
chloric1 - 28-7-2007 at 11:56
Shoot I wouldn't mind having a photo of the exploding cell