| I'd expect polyester fabric (PET plastic) to work better than cotton, however I posted a paper recently in this forum about using cross-linked
polyvinyl alcohol as an alkali-stable divided-cell membrane. Cross-linking can be done with gluteraldehyde solution (used to disinfect medical
devices) or by using periodate to cleave its occasional diol sites into aldehydes. PVA is subsidized by the Chinese government because it can be made
from coal instead of oil, so it's in practically everything. Clear dollar-store glue contains nothing else besides water, most of the time.
|