Gold Oxide
Hey, I have a tiny amount of gold (mainly scrap gold) and I want to turn it into gold oxide.
My first thought was to put it into solution with KNO3+HCl and then add sodium hydroxide/carbonate to precipitate gold hydroxide/carbonate which I
could then decompose into gold oxide.
But is it that simple or does the chloroauric acid complex not behave as straightforward as I hoped?
|
|
Motherload
Hazard to Others
Posts: 245
Registered: 12-8-2012
Location: Sewer
Member Is Offline
Mood: Shitty
|
|
And that would be energetic how ?
Also ... Aurous or Auric ?
Neutralization of Chloroauric acid with a alkali carbonate should form the hydrated Auric oxide..
Using carbonate will minimize the chance of forming complexes.
[Edited on 7-4-2013 by Motherload]
"Chance favours the prepared mind"
"Fuck It !! We'll do it live !!"
|
|
Tdep
National Hazard
Posts: 516
Registered: 31-1-2013
Location: Laser broken since Feb 2020 lol
Member Is Offline
Mood: PhD is done! It isn't good but it's over lol
|
|
Auric yeah. So adding a carbonate to chloroauric acid will create gold oxide, no gold carbonate formed?
Energetic?
|
|
weiming1998
National Hazard
Posts: 616
Registered: 13-1-2012
Location: Western Australia
Member Is Offline
Mood: Amphoteric
|
|
Quote: Originally posted by Tdep | Auric yeah. So adding a carbonate to chloroauric acid will create gold oxide, no gold carbonate formed?
Energetic? |
By itself, hydrated gold oxide is most probably not energetic (although it decomposes to oxygen and gold easily when heated). It can probably be used
to make energetic thermite mixtures with aluminium or magnesium, but it's not worth it. Better to use it, or finely-powdered gold, for non-energetic
purposes (e.g, as a catalyst for certain reactions)
[Edited on 7-4-2013 by weiming1998]
|
|
hissingnoise
International Hazard
Posts: 3940
Registered: 26-12-2002
Member Is Offline
Mood: Pulverulescent!
|
|
Fulminating gold?
|
|
Motherload
Hazard to Others
Posts: 245
Registered: 12-8-2012
Location: Sewer
Member Is Offline
Mood: Shitty
|
|
How much gold do you have and of what purity ?
I thought about fulminating gold but it hardly seems worth it.
"Chance favours the prepared mind"
"Fuck It !! We'll do it live !!"
|
|
aspiresquarelinks
Unregistered
Posts: N/A
Registered: N/A
Member Is Offline
|
|
Gold Oxide is a highly insoluble thermally stable Gold source suitable for glass, optic and ceramic applications. Two independent pathways for
corrosion of elements are hydrolysis and oxidation by oxygen. The combination of water and oxygen is even more corrosive.
|
|
Tdep
National Hazard
Posts: 516
Registered: 31-1-2013
Location: Laser broken since Feb 2020 lol
Member Is Offline
Mood: PhD is done! It isn't good but it's over lol
|
|
Well I was thinking about doing a gold thermite. That should be pretty energetic
Or is it really not worth the effort?
|
|
Finnnicus
Hazard to Others
Posts: 342
Registered: 22-3-2013
Member Is Offline
|
|
You gold potentially lose like 30-50$ of gold.
|
|
gregxy
Hazard to Others
Posts: 421
Registered: 26-5-2006
Member Is Offline
Mood: No Mood
|
|
Gold thermite???
I don't think you will get much bang for your buck.
(sorry, I couldn't resist).
|
|
elementcollector1
International Hazard
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Not worth it, in both the monetary and empirical sense. Gold thermite will look like every other thermite, and if the thermite was big enough, there
might be some molten gold in your crucible afterwards.
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
Tdep
National Hazard
Posts: 516
Registered: 31-1-2013
Location: Laser broken since Feb 2020 lol
Member Is Offline
Mood: PhD is done! It isn't good but it's over lol
|
|
Aww maybe not then, that pun has disheartened me quite a bit haha. Thought it would be the most viloent thermite, becuase of gold's low reactivity?
[Edited on 9-4-2013 by Tdep]
|
|
Motherload
Hazard to Others
Posts: 245
Registered: 12-8-2012
Location: Sewer
Member Is Offline
Mood: Shitty
|
|
It maybe violent .... But you can similar results with lot less with CuO thermite or flash powder.
"Chance favours the prepared mind"
"Fuck It !! We'll do it live !!"
|
|
Tdep
National Hazard
Posts: 516
Registered: 31-1-2013
Location: Laser broken since Feb 2020 lol
Member Is Offline
Mood: PhD is done! It isn't good but it's over lol
|
|
Of course but.... gold.. thermite... ah fine. I give up.
But the fulminating gold looks fascinating! There a thread for this already?
|
|
Motherload
Hazard to Others
Posts: 245
Registered: 12-8-2012
Location: Sewer
Member Is Offline
Mood: Shitty
|
|
Ok ok ... You want to try Gold thermite. Lets try 2 experiments in one ....
How about you also cover a small quantity with a a small beaker or similar .... To see if gold vapor will deposit itself on the glass. Quartz/Gold
mirrors are more efficient in reflecting infra red than standard mirrors.
Also this way you might some of your gold back..
"Chance favours the prepared mind"