Make Calcium carbonate from calcite
Hi All
I have some Calcite and I wanted to purify calcium carbonate from it. What would you suggest is the best way to do this.
Thanks
Housane
|
|
Foeskes
Hazard to Others
 
Posts: 156
Registered: 25-2-2017
Member Is Offline
Mood: No Mood
|
|
Well if it's clear or white, then I'd say it's pretty pure especially if it's in the form of large crystals.
|
|
Housane
Hazard to Others
 
Posts: 127
Registered: 3-9-2018
Location: Worcester, England
Member Is Offline
Mood: Let’s make
|
|
Hi how can I then make it into a powdered form to make calcium hydroxide what would you subject is best. The chunks are rather large
|
|
fusso
International Hazard
   
Posts: 1907
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline
|
|
Just heat it up to 8xxC to form CaO. The pressure from released CO2 will break the chunks apart.
|
|
Ubya
International Hazard
   
Posts: 1213
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
Quote: Originally posted by fusso  | Just heat it up to 8xxC to form CaO. The pressure from released CO2 will break the chunks apart. |
then add water and a slurry of calcium hydroxide will form (be careful of the exothermic reaction)
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
If you are looking for chemicals check this out: [For Sale]300 chemicals (rare & unusual)
---------------------------------------------------------------------
|
|
Housane
Hazard to Others
 
Posts: 127
Registered: 3-9-2018
Location: Worcester, England
Member Is Offline
Mood: Let’s make
|
|
Hi Ubya how did you get the part at the bottom
|
|
fusso
International Hazard
   
Posts: 1907
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline
|
|
Filtering.
|
|
MrHomeScientist
International Hazard
   
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
Well calcite is already calcium carbonate, so smash it with a hammer and you're done!
If you want to ensure purity, probably the easiest way would be:
1) Crush the rock as much as you can with a hammer / mortar & pestle.
2) Dissolve the rock in vinegar. May take a few hours or days; wait until the bubbling stops, then add a bit more vinegar and make sure bubbling
doesn't start up again.
3) Filter off any undissolved rock. The solution contains calcium acetate.
4) Add baking soda to the solution. This precipitates the calcium back out as carbonate.
4a) It might be better to first dissolve the baking soda in its own solution, then add that to the acetate solution. This way you know the
precipitation is done if you add baking soda solution and no more is observed.
|
|