[*] posted on 29-1-2019 at 07:47
Chemistry with terracotta pots - what are some experiments that can be done?


I remember reading some time back that terracotta can be used in various types of chemistry, possibly electrolysis or filtration, I don't remember. I know the standard pots with the hole in the bottom often creates a problem and if the hole can be properly plugged or is absent, it makes the process much better/easier. Maybe it is used as a membrane or something (possibly to make NaOH/KOH from their respecitve salts?

I've been talking to a potter and they will make custom pots in whatever size I need for a good price.

What are some good experiments that can be done with terracotta that would be worthwhile doing?

I'm very interested in finding as many examples as possible b/c I'm planning on doing a research and instructional series for high school and college students, so hopefully they can replicate the same experiments on their own.

What are some experiments that can be done - don't discount experiments that require even semi-exotic compounds as I'm looking at making a large list of experiments to carry out.
View user's profile View All Posts By User
Ubya
International Hazard
*****




Posts: 711
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 29-1-2019 at 09:07


it can be used as cell membrane as you said
boiling stones
catalyst support
cracking of hydrocarbons catalyst (like allumina)

at the moment i can think only of these





---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 4677
Registered: 4-10-2014
Location: Oz
Member Is Offline

Mood: Metastable, and that's good enough.

[*] posted on 29-1-2019 at 14:29


They are the container of choice for thermite reactions.
View user's profile View All Posts By User
vmelkon
International Hazard
*****




Posts: 637
Registered: 25-11-2011
Location: Canada
Member Is Offline

Mood: autoerotic asphyxiation

[*] posted on 29-1-2019 at 15:12


Quote: Originally posted by Ubya  
it can be used as cell membrane as you said
boiling stones
catalyst support
cracking of hydrocarbons catalyst (like alumina)

at the moment i can think only of these


Does the cracking of hydrocarbons work? Has anybody tried it?




Signature ==== Is this my youtube page? https://plus.google.com/u/0/102731756100318541546/videos?tab...
We must attach the electrodes of knowledge to the nipples of ignorance and give a few good jolts.
Yes my evolutionary friends. We are all homos here.
View user's profile View All Posts By User
Ubya
International Hazard
*****




Posts: 711
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 29-1-2019 at 17:10


Quote: Originally posted by vmelkon  
Quote: Originally posted by Ubya  
it can be used as cell membrane as you said
boiling stones
catalyst support
cracking of hydrocarbons catalyst (like alumina)

at the moment i can think only of these


Does the cracking of hydrocarbons work? Has anybody tried it?


https://youtu.be/7M7RY04KKBs

(i'll try once i can get some free time)





---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
View user's profile View All Posts By User
Simoski
Hazard to Self
**




Posts: 69
Registered: 24-12-2017
Location: Johannesburg South Africa
Member Is Offline

Mood: No Mood

[*] posted on 29-1-2019 at 21:23


You can make perchlorates and chlorates using a divided cell. In a way it simplifies the chemistry, because instead of a whole bunch of reactions going on in an undivided cell, in a divided cell you have 2 simpler reactions occuring. It allows more control.

Maybe a professional chemist could comment on such with an example....

8 )




View user's profile View All Posts By User
MrHomeScientist
International Hazard
*****




Posts: 1760
Registered: 24-10-2010
Location: Flerovium
Member Is Offline

Mood: No Mood

[*] posted on 30-1-2019 at 06:36


As others mentioned, I've used one as a membrane in an electrolysis cell to make NaOH from NaCl. Let it soak in the solution for a while to reach full conductivity. The hard part is sealing the hole in the bottom with something that is resistant to both hydroxide and chlorine. I used caulk but that failed after a few hours.
View user's profile Visit user's homepage View All Posts By User
monolithic
Hazard to Others
***




Posts: 126
Registered: 5-3-2018
Member Is Offline

Mood: No Mood

[*] posted on 2-2-2019 at 13:56


Quote: Originally posted by MrHomeScientist  
As others mentioned, I've used one as a membrane in an electrolysis cell to make NaOH from NaCl. Let it soak in the solution for a while to reach full conductivity. The hard part is sealing the hole in the bottom with something that is resistant to both hydroxide and chlorine. I used caulk but that failed after a few hours.


I've heard that plumber's putty (the stuff used to seal around drains in sinks) holds up better. I might try it myself, using a plain flower pot. The biggest concern is that the pot is too thick. Sanding it down by hand is pretty much an impossible task.
View user's profile View All Posts By User
monolithic
Hazard to Others
***




Posts: 126
Registered: 5-3-2018
Member Is Offline

Mood: No Mood

[*] posted on 3-2-2019 at 05:00


Yeah, plumber's putty is out if you're using acidic electrolytes. It lasted less than 5 minutes with a dilute sulfuric acid solution.
View user's profile View All Posts By User
Ubya
International Hazard
*****




Posts: 711
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 3-2-2019 at 05:13


has anyone tried sodium silicate and sand to fill the hole? after exposure to heat or CO2 it hardens




---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
View user's profile View All Posts By User
pomegranate
Harmless
*




Posts: 10
Registered: 13-12-2018
Member Is Offline


[*] posted on 27-2-2019 at 14:45
Iridium compounds?


what do you think of this?

i was wondering about some day, fusing iridium powder with K2CO3 in hopes of getting Potassium oxide or Potassium superoxide
by using a oxy propane torch, set with an O2 heavy oxydizing flame or with oxy acetylene, set with exess O2

hopefully that would make K2IrO3 and KIrO3

https://en.m.wikipedia.org/wiki/Iridium
“Iridium also forms iridates with oxidation states +4 and +5, such as K2IrO3 and KIrO3, which can be prepared from the reaction of potassium oxide or potassium superoxide with iridium at high temperatures.[20]”

[20] Gulliver, D. J.; Levason, W. (1982). "The chemistry of ruthenium, osmium, rhodium, iridium, palladium and platinum in the higher oxidation states". Coordination Chemistry Reviews. 46: 1–127. doi:10.1016/0010-8545(82)85001-7.
View user's profile View All Posts By User
symboom
International Hazard
*****




Posts: 801
Registered: 11-11-2010
Location: Wrongplanet
Member Is Offline

Mood: Doing science while it is still legal since 2010

[*] posted on 27-2-2019 at 18:32


as i seen on the permanganates thread success has been made using terracotta pots to keep the potassium permanganate from being reduced by the cathode
http://www.sciencemadness.org/talk/viewthread.php?tid=8480&a...

[Edited on 28-2-2019 by symboom]




Chemistry video Storage
https://www.mediafire.com/folder/kbll6gz9bdb4q/Videos
The State of Mad Science newsletter
http://www.sciencemadness.org/talk/viewthread.php?tid=98577
My open source scratch paper
Pastebin.com/u/symboom
Natures Intellectual Organic Peroxide. >>Ascaridole <<
2020 year of science
Oxone
Used for the production of --> CH2O/Cl2/ClO2/Br2/I2
------------------------------------->>Hydrogen Peroxide <<
Sodium had its fame long enough time for Calcium
View user's profile View All Posts By User