nitrogen content of "magicians flash paper"


I was wondering what is the nitrogen content of the flash paper marketed as a tricksters item. It seems to leave no residue upon combustion but that's not a good indication of the degree of nitration. Has anyone here compared high quality homemade nc with this stuff or could otherwise share some knowledge?
View user's profile View All Posts By User
MineMan
National Hazard
****




Posts: 383
Registered: 29-3-2015
Member Is Offline

Mood: No Mood

[*] posted on 15-3-2019 at 16:49


12 percent is about what they use. Homemade can have more.