Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Allotropes of Sulpher
Wrecking Bereserker
Harmless
*




Posts: 25
Registered: 2-4-2019
Member Is Offline


[*] posted on 2-4-2019 at 08:28
Allotropes of Sulpher


I'm trying to make allotropes of sulpher but not getting it right these are steps i took help me through it
I tried to dissolve sulpher in CCl4 and heat to evaporate to produce sulphur crytals it didn't work
Then heated a new sample it until it melts and poured it into cold water wich made some tiny balls i don't quite sure what to do after that
Then i heated an another sample until it became sticky this is also an allotrope right?
View user's profile View All Posts By User
12thealchemist
Hazard to Others
***




Posts: 181
Registered: 1-1-2014
Location: The Isle of Albion
Member Is Offline

Mood: Rare and Earthy

[*] posted on 2-4-2019 at 08:39


There are many allotropes of sulphur. Rhombic and monoclinic are the most common. Rhombic sulphur is stable at room temperature, and is the most stable allotrope. Monoclinic sulphur is only stable above 95.3°C, and can be prepared by crystallising sulphur at 100°C. Plastic or amorphous sulphur (μ-sulfur) can be prepared by pouring sulphur heated to above 160°C into water. It is unstable, and over a few days will slowly revert to rhombic sulphur.
λ-sulphur is the light yellow liquid formed when sulphur initially melts
π-sulphur is formed when λ-sulphur is allowed to sit just above the melting point for an extended period of time. It is a dark colour.
Trisulphur is present in hot boiling sulphur vapour, and is visible as a dark red gas.




Just my two pennyworth
My YouTube channel: www.youtube.com/channel/UC4t9tVlAk7ww1wgCVW4yUjg
Elements collected so far: 65; to collect: Ln, Rb, Sr, Ba, F, Kr, radioactives
View user's profile Visit user's homepage View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3228
Registered: 8-2-2015
Location: UK ... on extended Holiday in Malaysia
Member Is Offline


[*] posted on 2-4-2019 at 08:55


Sulphur is not very soluble in CCl4, 0.8 % w/w
Attachment: Solubilityofelementalsulfur.pdf (42kB)
This file has been downloaded 2503 times
so you would have to make a saturated solution, filter it and DISTILL off the CCl4 as the fumes are a health hazard.

CS2 dissolves sulphur easily but is not cheap and its fumes are also undesirable.

I have grown sulphur crystals from sulphur dissolved in toluene,
but the solubility is also quite low, which means wasting valuable solvent (and polluting the air)
or distillation which is a nuisance to set up for a simple experiment.




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 7736
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 2-4-2019 at 23:01


Sulphur dissolves quite well in hot toluene, not in cold toluene. I once dissolved some sulphur in toluene, kept at around 100 C and then allowed the toluene to cool down slowly. I put the test tube with a saturated solution of sulphur in hot toluene in a beaker, which I filled with boiling hot water. I used a glass tea beaker, which is double-walled, with low pressure between the two glass walls. These beakers keep the liquid warm for quite some time. In this way, I could make nice shiny crystals of sulphur.



The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
Tsjerk
International Hazard
*****




Posts: 2783
Registered: 20-4-2005
Location: Netherlands
Member Is Offline

Mood: Mood

[*] posted on 3-4-2019 at 06:40


I made some really nice slightly yellow needles of sulfur by crystallization from hot toluene.
View user's profile View All Posts By User
12thealchemist
Hazard to Others
***




Posts: 181
Registered: 1-1-2014
Location: The Isle of Albion
Member Is Offline

Mood: Rare and Earthy

[*] posted on 3-4-2019 at 08:44


I've also recrystallised sulphur from toluene to excellent effect - it's fairly soluble in boiling toluene, far far less so in cold. And since toluene is impossible to freeze without LN2, you can chill it right down to squeeze out almost all the sulphur you do dissolve.



Just my two pennyworth
My YouTube channel: www.youtube.com/channel/UC4t9tVlAk7ww1wgCVW4yUjg
Elements collected so far: 65; to collect: Ln, Rb, Sr, Ba, F, Kr, radioactives
View user's profile Visit user's homepage View All Posts By User

  Go To Top