[*] posted on 20-4-2019 at 05:56
Stainless steel


Hi.

Is stainless steel resistant to copper sulfate and strong acids?
View user's profile View All Posts By User
fusso
International Hazard
*****




Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline


[*] posted on 20-4-2019 at 06:12


No, it will dissolve in HCl.



View user's profile View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1235
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 20-4-2019 at 06:17


Thank you.
View user's profile View All Posts By User
Felab
Hazard to Self
**




Posts: 76
Registered: 9-11-2018
Member Is Offline

Mood: :dooM

[*] posted on 20-4-2019 at 08:13


It depends on which type of stainless steel. 316 stainless steel will resist HCl for example.