Hazards79
Harmless
Posts: 6
Registered: 23-8-2019
Member Is Offline
|
|
Home made stainless steel pressure vessel
I’m looking for any advice or tips for making a 10 litre stainless steel pressure vessel that will be safe for basic chemical reactions. I’m a
welder so that won’t be an issue I’m just after any hints or tricks from someone who has travelled this path
|
|
|
draculic acid69
International Hazard
   
Posts: 1371
Registered: 2-8-2018
Member Is Offline
|
|
I've never done this but I have looked into doing it and there's something like asme 8 classes that welders take to get trained in making hi psi
vessels. It's really a dangerous thing to do so planning it well is essential.will you need to heat the rxn vessel while under pressure?these vessels
can be bought cheaply on eBay though not in that size. It might be acms not asme I can't remember but its one of the two.
|
|
|
Abromination
Hazard to Others
 
Posts: 432
Registered: 10-7-2018
Location: Alaska
Member Is Offline
Mood: 1,4 tar
|
|
What basic reactions are you planning to do under pressure? This is a very dangerous thing to attempt in a home lab and even more so to use a homemade
one. If you do it, take every precaution possible. Work behind a clear shatter proof plastic shield, wear thick clothing to prevent getting hit by
shrapnel, check everything more then once and stay away from it when possible. Leave windows open all the way or work outside.
List of materials made by ScienceMadness.org users:
https://docs.google.com/spreadsheets/d/1nmJ8uq-h4IkXPxD5svnT...
--------------------------------
Elements Collected: H, Li, B, C, N, O, Mg, Al, Si, P, S, Fe, Ni, Cu, Zn, Ag, I, Au, Pb, Bi, Am
Last Acquired: B
Next: Na
--------------
|
|
|
Fantasma4500
International Hazard
   
Posts: 1682
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline
Mood: dangerously practical
|
|
i would suggest flange connection at top, this may be made by taking 2 pieces of steel plate, welding sides, drilling holes. super cheap solution you
dont even bother threading one of the plates (i suppose threading both plates would be counterproductive) but instead just tightening it with bolts
i recall its something around several tonnes one single 14mm bolt can hold, AvE made a simple bolt-press this way, then you would want a sealant,
silicone rubber would be ideal here, i think MAYBE some soft metal can be used if it can resist the chemicals?
i would also suggest welding in some flat bar steel rods or similar, inside of the container to strenghten it, also on the bottom
of course welding you would wanna use backing gas to prevent it corroding on the inside, butane might work. may just turn into carbon which would
then require cleaning. imo more diy than helium regardless
the opening could also maybe be just a bolt in the side, but it would probably require silicone rubber every time you need to use it, maybe some
silicone grease could work.
to prevent the whole thing fragmenting if it does burst you could attach some external frame or just weld some steelpieces on the sides attached to
the bottom
it would of course be ideal to chamfer all the connections youre making before welding so you get 100% penetration without doubt, honestly a bunch of
welding is totally overrated, welding is just held to such high standards so they cant blame the metalworkers when some drunk crane driver fucks up
i would suggest bottom plate to be smaller diameter than the pipe and pushed maybe 20mm into the pipe to be welded, mechanical leverage physics kinda
thing
|
|
|
MrHomeScientist
International Hazard
   
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
What sort of "hints or tricks" are you looking for? If you're a welder with pressure certification, you surely know more about that side than we do.
If you're asking about chemistry advice, you'd do well to refer back to your other thread. I hope this new thread isn't an attempt to distance
yourself from the safety advice given over there. You asked about the chemistry, and people gave you very reasonable answers. We're just trying to
help.
If you want more concrete evidence, here's a chemical compatability chart for stainless: http://www.quickcutgasket.com/pdf/Chemical-Resistance-Chart....
It doesn't have HI, but it lists iodine as "Severe effect - not recommended". Several other charts I found agree. It looks like about the only metal
that works is titanium.
|
|
|
Fantasma4500
International Hazard
   
Posts: 1682
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline
Mood: dangerously practical
|
|
it may be possible to coat the stainless steel with glass using sodium silicate, had a very sturdy layer of glass on stainless steel pot when i let
some sodium silicate evaporate to dryness at around 60*C
|
|
|