beerwiz
Hazard to Others
***




Posts: 123
Registered: 6-2-2014
Member Is Offline

Mood: No Mood

[*] posted on 10-11-2019 at 23:21
How to make HAuCl4.3H2O?


Every time I try to make HAuCl4.3H2O I get the red crystalline (red garnet looking) AuCl3. After all the Au is dissolved, I heat the AR solution in a sand bath at 225°C to evaporate it. The temperature must be too high and it converts to the red AuCl3 instead. Although I've tried evaporating at 100°C and it still turns to blood red AuCl3.

Any suggestions on how to get perfect and dry HAuCl4.3H2O crystals quickly?

View user's profile View All Posts By User
Deathunter88
National Hazard
****




Posts: 464
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline

Mood: No Mood

[*] posted on 11-11-2019 at 08:05


Place in a sealed bag of NaOH.
View user's profile View All Posts By User
beerwiz
Hazard to Others
***




Posts: 123
Registered: 6-2-2014
Member Is Offline

Mood: No Mood

[*] posted on 11-11-2019 at 18:46


How long does it take to dry up with NaOH in a sealed bag?
View user's profile View All Posts By User