Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Removing orange dye from sodium silicate solution?
Draeger
Hazard to Others
***




Posts: 185
Registered: 31-1-2020
Location: North-Rhine Westfalia, Germany
Member Is Offline

Mood: Slowly getting ready for new projects

[*] posted on 29-4-2020 at 06:03
Removing orange dye from sodium silicate solution?


So, I wanted to make some sodium silicate by dissolving silica gel pearls in sodium hydroxide. I only had orange dyed pearls, though, so now the dye is dissolved in the water. Is there any way to separate the dye from the product? According to Wikipedia, the dye is methyl violet, by the way.



Collected elements:
Al, Cu, Ga, C (coal), S, Zn, Na

Collected compounds:

Inorganic:
NaOH; NaHCO3; MnCl2; MnCO3; CuSO4; FeSO4; aq. 30-33% HCl; aq. NaClO; aq. 9,5% ammonia; aq. 94-96% H2SO4; aq. 3% H2O2

Organic:
citric acid, sodium acetate, sodium citrate, petroleum, mineral oil
View user's profile View All Posts By User
SWIM
National Hazard
****




Posts: 970
Registered: 3-9-2017
Member Is Offline


[*] posted on 29-4-2020 at 14:15


Many dyes adhere pretty strongly to activated charcoal, you might be able to adsorb it.

If you have an ozone source maybe you could oxidize it away?
Shouldn't hurt the sodium silicate any.

Maybe H2O2?

Sodium silicate should be able to take lots of heat, so maybe you could burn the dye out like burning the organics out of potash.




View user's profile View All Posts By User
formallydehyde
Harmless
*




Posts: 5
Registered: 6-4-2020
Member Is Offline


[*] posted on 29-4-2020 at 22:34


If you can't get the undyed silica gel for some reason, I agree with SWIM's suggestion to try hydrogen peroxide, since that could just be removed by heating. That sounds like it would be the easiest way if you can't start over with new gel.

I use concentrated bleach to remove crystal violet (one of the methyl violets) from glassware pretty often and it's effective for that, but I can't think of a great way that sodium hypochlorite could be removed safely and without generating a soluble salt.
View user's profile View All Posts By User
AJKOER
Radically Dubious
*****




Posts: 3026
Registered: 7-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 1-5-2020 at 17:07


Add B-12 or B-Complex and even better, add nano-ZnO (at home prepared, no less, see https://ninithi.wordpress.com/2015/08/06/make-your-own-photo... ).

Now, more colorful!

Let sunlight work on it, and alas colorless!! Source: https://jurnal.ugm.ac.id/ijc/article/view/33470/20955 .

Assuming Sodium silicate will resist attack by radicals, but if it is that would also be interesting!!!

[Edited on 2-5-2020 by AJKOER]
View user's profile View All Posts By User
draculic acid69
International Hazard
*****




Posts: 1371
Registered: 2-8-2018
Member Is Offline


[*] posted on 2-5-2020 at 02:26


What about burning it out or acetone/solvent wash
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5104
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 2-5-2020 at 05:34


I suspect that you might be trying to remove Fe(III) by oxidation.
Good luck.
https://patents.google.com/patent/US8247237B2/en

It might be instructive to do a weak acid wash on some of the original gel.

[Edited on 2-5-20 by unionised]
View user's profile View All Posts By User