PTFE powder from granules


As per subject really, i have some Shamrock PTFE granules that i'd like to grind/chop/mash/bully into powder form.

Any Ideas ??
View user's profile View All Posts By User
draculic acid69
International Hazard
*****




Posts: 1371
Registered: 2-8-2018
Member Is Offline


[*] posted on 21-5-2020 at 05:38


The best idea is buy the powder off eBay as trying to powder any sort of plastic is gunna be extremely hard and not very effective
View user's profile View All Posts By User
Steve s
Harmless
*




Posts: 46
Registered: 20-2-2019
Member Is Offline


[*] posted on 21-5-2020 at 13:03


Yeah i do have some already in powder form, just happened to acquire this as part of a job lot and the only thing i can think of to do with it is PTFE Al rocket motors.
Although thinking about it, it might work well in a reflux column.
View user's profile View All Posts By User
Herr Haber
International Hazard
*****




Posts: 1236
Registered: 29-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 23-5-2020 at 10:15


I'd go the eBay route too.

Though if I had dry ice maybe... wait, I just checked Youtube for the idea that was sprouting in my brain and found nothing :)

I'll be damned. Usually when I have a silly idea someone always thought of it and posted a video about it on Youtube before.
(Sometimes a SM member)

I was thinking about freezing it with liquid nitrogen or dry ice and then try to crush the granules with anything from a potato masher or the usual mortar.
You wouldnt get a regular granularity but it could be fun to try.




The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
View user's profile View All Posts By User
Steve s
Harmless
*




Posts: 46
Registered: 20-2-2019
Member Is Offline


[*] posted on 23-5-2020 at 12:21


Quote: Originally posted by Herr Haber  
I'd go the eBay route too.

Though if I had dry ice maybe... wait, I just checked Youtube for the idea that was sprouting in my brain and found nothing :)

I'll be damned. Usually when I have a silly idea someone always thought of it and posted a video about it on Youtube before.
(Sometimes a SM member)

I was thinking about freezing it with liquid nitrogen or dry ice and then try to crush the granules with anything from a potato masher or the usual mortar.
You wouldnt get a regular granularity but it could be fun to try.


Worth a try. Pretty sure dry ice wouldn't get it cold enough but LQN might.