Large Quartz Tubes For Cheap? - Patio Heater


Hi All,

In my search for quartz tubes I've come across quite a few sellers online selling "quartz" glass tubes for the commonly sold pyramid style propane patio heaters. They are 4" in diameter, and nearly 50" long for only about $80 USD. Assuming these are genuine quartz tubes, it could be one hell a deal. I am looking to build a tube furnace, and despite this being way bigger than I initially wanted to build, it may make alot more economic sense.

Can anyone verify that these tubes are actually quartz and not just borosilicate? I already messaged a seller, and they said it is quartz, but I'm not sure I trust how well amazon sellers actually know the technical details of their products.

Also, are there any simple non-destructive tests to test for quartz vs borosilicate glass? I may just order a few of these tubes, and test them to see if they are quartz or not, and would rather not break them so I could return them.

[Edited on 18-3-2021 by BobD1001]
View user's profile Visit user's homepage View All Posts By User
Twospoons
International Hazard
*****




Posts: 1174
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline

Mood: A trace of hope...

[*] posted on 17-3-2021 at 16:20


See if it will pass short UV light. If it does then its quartz.

[Edited on 18-3-2021 by Twospoons]




Helicopter: "helico" -> spiral, "pter" -> with wings
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1558
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 17-3-2021 at 16:28


If you tune in starting a little after the 14:30 mark there's this Applied Science cautionary tale.
https://youtu.be/Xr1AiExSAnU

And this. I guess they make both but replacement tubes might be boro depending on the source and most likely the cost.
https://youtu.be/xyUtriix_N0

There are these and other shapes made for UV bulbs that are not too expensive.
https://youtu.be/ddqYSZd29a4
View user's profile View All Posts By User
RustyShackleford
Hazard to Others
***




Posts: 173
Registered: 10-12-2020
Location: Northern Europe
Member Is Offline


[*] posted on 17-3-2021 at 17:06


Quote: Originally posted by Morgan  

There are these and other shapes made for UV bulbs that are not too expensive.
https://youtu.be/ddqYSZd29a4

I wasnt aware there was decent size quartz glass for such good prices. Fortunately even though the video is old, the tubes seem to still be available on ebay.
View user's profile View All Posts By User
macckone
International Hazard
*****




Posts: 2126
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 17-3-2021 at 19:22


The quartz used in patio heaters is usually of a 96% silica.
It is somewhere between common 3.3 borosilicate and fused quartz.
The shock resistance is similar and the softening point only differs by about 80C from fused quartz.
The expansion also very similar 0.750um/m degree C compared to 0.700um/m degree C.
They are similar enough that standard taper joints don't need special handling.