Quote: Originally posted by vano  
Hi. I made cobalt selenite again and also anhydrous selenite.

Those are spectacular colors! How did you make them? Do you have a procedure posted in another thread? I'd like to try this myself.
View user's profile Visit user's homepage View All Posts By User
vano
International Hazard
*****




Posts: 660
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 1-6-2022 at 07:18


Quote: Originally posted by vano  

also, cobalt selenite precipitation is a little bit hard than Cu and Ni selenites. I dissolved sodium selenite and cobalt chloride hydrates in hot water. then I mixed the solution but nothing precipitated, then I poured the mixture into another beaker and there was cold water. then it precipitated instantly. From my experience, you cant make the compound with a high yield just dissolve compounds in hot or cold water and mix them.


Hi. this is the procedure.




View user's profile View All Posts By User
vano
International Hazard
*****




Posts: 660
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 1-6-2022 at 07:19


Selenium dioxide.

280985062_393147329406951_4790574120533607550_n.jpg - 310kB




View user's profile View All Posts By User
vano
International Hazard
*****




Posts: 660
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 9-6-2022 at 11:26


Caesium hexabromoselenite.

281846504_4835478666581292_2539160779596896814_n.jpg - 264kB




View user's profile View All Posts By User
vano
International Hazard
*****




Posts: 660
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 21-9-2022 at 07:01
TITANIUM SELENITE(?)


We know that many compounds of Ti(III) are unstable, for example hydroxide, tungstate... but yesterday i mix some titanium trichloride and sodium selenite solutions, it is logical to think that titanium can reduce selenite to red selenium in the solution. but when I tried this reaction in a test tube it wasn't red allotropy.

i made more, then i filtered it and put on petri dish, i can dry it with other methods, but i use sunlight, because if there was any red selenium or it was red selenium precipitate it must turn black color. onced i tryed to dry red alotropy under sunlight and it takes 30 minute to be black.

unfortunately i couldn't find any info about trivalent selenite.



IMG-2373.jpg - 3.4MB
IMG-2376.jpg - 1.4MB
IMG-2380.jpg - 1.3MB




View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 7816
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 22-9-2022 at 00:28


Maybe the reduction by titanium(III) is so vigorous, that the selenium is reduced all the way down to selenide. That would lead to TiSe2. I don't know the properties of that.



The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
vano
International Hazard
*****




Posts: 660
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 22-9-2022 at 05:37


I'm not sure 100% about what it is, These are just my assumptions. bad thing is that I couldn't find any info. so ill put all of my powder in nitric acid and make some titanium dioxide hydrate. I have TiO2 but you know it's very inert, because of its calcinated temperature. and ill make some Ti(IV) complexes, just more logical valency to work with.



View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2439
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 22-9-2022 at 05:50


Selenides of titanium may be alloy-like, TiSex, rather than salt-like. Selenium is not terribly electronegative. TiS2 is a conductor IIRC.



[Edited on 04-20-1969 by clearly_not_atara]
View user's profile View All Posts By User
vano
International Hazard
*****




Posts: 660
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 22-9-2022 at 06:18


yes, many possible formulas, selenide, polyselenide, selenite, and different valency of titanium... unfortunately I can't make an analysis now. but worth to try I think, but I don't recommend it for forum members. I just hate when I have chemical and I don't know exactly what it is. thanks, everyone for your ideas!