Author: Subject: so much bubbles in glass
dioxine
Harmless
*




Posts: 13
Registered: 17-12-2018
Member Is Offline


[*] posted on 21-5-2021 at 06:17
so much bubbles in glass


Well, i had some glass from china that was not that bad, but with some defects so i decided to buy some glass from local russian store which was(as i thought) reliable. I thought it will be russian manufacturer like "Klin" which is good. When glass came what i saw is literally chinese glass with russian label on it. And it has so much bubbles!

It is that bad for regular use? (Not for vaccum or something like that). Photos attached.



[Edited on 21-5-2021 by dioxine]

[Edited on 21-5-2021 by dioxine]
View user's profile View All Posts By User
njl
International Hazard
*****




Posts: 584
Registered: 26-11-2019
Location: under the sycamore tree
Member Is Offline

Mood: ambivalent

[*] posted on 21-5-2021 at 06:23


I'd really avoid putting much stress on that joint, and distillations where the vapor front moves slowly and has a high temperature gradient. For example taking off a high boiling solvent where a very hot vapor front moves discretely up the stillhead and heats one side of the joint before the other.



Reflux condenser?? I barely know her!
View user's profile View All Posts By User
dioxine
Harmless
*




Posts: 13
Registered: 17-12-2018
Member Is Offline


[*] posted on 21-5-2021 at 06:25


Thanks nij. Think i should try this one with water distillation to see if something will happen.
View user's profile View All Posts By User
zed
International Hazard
*****




Posts: 2247
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline

Mood: Semi-repentant Sith Lord

[*] posted on 25-5-2021 at 21:38


Ummm. I'm in the USA.

I assume that the expensive high quality American Glassware, available here... Is actually made in China.

The American Corporations involved, pay slightly more, and exercise stringent quality control.

If you are paying a premium for "Russian" Glassware, you should be getting premium Russian Quality.

We buy plenty of Chinese Glassware around here. Quality isn't really great, but it is dirt cheap. Which is OK.

Not OK, is expecting high quality, and getting glassware full of bubbles.

View user's profile View All Posts By User
draculic acid69
International Hazard
*****




Posts: 1256
Registered: 2-8-2018
Member Is Offline


[*] posted on 26-5-2021 at 01:52


Send it back and tell them it's unnaceptable. Try and get a refund
View user's profile View All Posts By User
dioxine
Harmless
*




Posts: 13
Registered: 17-12-2018
Member Is Offline


[*] posted on 8-6-2021 at 11:45


our amauter-chemists market is really that small so there is only few shops and they often don't care about quality or service so this is gonna be waste of my time if i try to send it back.
No choise really, there is no different shops with "Premium" quallty.

[Edited on 8-6-2021 by dioxine]
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 4768
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 9-6-2021 at 02:57


It's obviously not ideal, but that glassware survived the thermal gradients involved in the manufacturing process.
So it is quite likely to survive those encountered in use.
Also, glass is a lot stronger and more flexible than most people give it credit for.


And
Quote: Originally posted by dioxine  
When glass came what i saw is literally chinese glass with russian label on it.



Do you know what "literally" means?
View user's profile View All Posts By User
Clear_horizons_glass
Harmless
*




Posts: 35
Registered: 30-9-2019
Location: Pullman, WA
Member Is Offline

Mood: Glass

[*] posted on 25-6-2021 at 09:46


Scientific glassblower here. If ya want something made without bubbles, message me. That apparatus looks easy enough to replicate.



Clear Horizons Laboratory Glassblowing Services
-------------------------------------------------------------
www.clearhorizonsglass.com
Phone and Fax:
(855) LAB-GLAS
(855) 522-4527
Have a glass project you want made? email me at
info@clearhorizonsglass.com
or message us here |
with a U2U |
message |
\/
View user's profile Visit user's homepage View All Posts By User

  Go To Top