Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: How do I make Lactic Acid from Polylactic Acid?
9CWAI
Harmless
*




Posts: 16
Registered: 5-2-2019
Location: Utah
Member Is Offline


[*] posted on 8-1-2022 at 21:49
How do I make Lactic Acid from Polylactic Acid?


I have lots of PLA waste from a 3d printer and no hotplate so I cannot temperature control enough to not burn it when melting it. I want to make Lactic acid from it but boiling for a while did little but warp it. How can I encourage the water to attack the PLA?
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4504
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 8-1-2022 at 22:10


You should be able to hydrolyze it with strong base to get lactate ion, then acidify to get lactic acid.



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
SaccharinSlayer157
Harmless
*




Posts: 30
Registered: 1-10-2020
Location: Near Cou?
Member Is Offline

Mood: Resisting the urge to build a ketene lamp

[*] posted on 8-1-2022 at 22:24


Well, I was going to say something about that but apparently I'm wrong, so nevermind :P

[Edited on 9-1-2022 by SaccharinSlayer157]
View user's profile View All Posts By User
9CWAI
Harmless
*




Posts: 16
Registered: 5-2-2019
Location: Utah
Member Is Offline


[*] posted on 9-1-2022 at 14:19


Quote: Originally posted by DraconicAcid  
You should be able to hydrolyze it with strong base to get lactate ion, then acidify to get lactic acid.

What would you recommend out of the easily obtainable 3, Ca(OH)2, NaOH, or KOH? which one would be the easiest to get rid of?
View user's profile View All Posts By User
9CWAI
Harmless
*




Posts: 16
Registered: 5-2-2019
Location: Utah
Member Is Offline


[*] posted on 9-1-2022 at 14:24


I really don't wanna use H2SO4.
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4504
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 9-1-2022 at 16:48


If you use calcium hydroxide, then you can neutralize with sulphuric or phosphoric acid, filter out the calcium salts, and have a fairly pure solution of lactic acid. If you acidify with a different acid (such as hydrochloric), then regardless of which base you use, you'll want to have an excess of base so that you can distill the lactic acid (ew!) without any excess acid coming over.

Just hypothesizing here, but you might also be able to hydrolyze the polymer by refluxing it in aqueous acid for a while, adding just enough bicarbonate to neutralize the acid that you've added, and then distilling.




Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
9CWAI
Harmless
*




Posts: 16
Registered: 5-2-2019
Location: Utah
Member Is Offline


[*] posted on 10-1-2022 at 17:05


Quote: Originally posted by DraconicAcid  
If you use calcium hydroxide, then you can neutralize with sulphuric or phosphoric acid, filter out the calcium salts, and have a fairly pure solution of lactic acid. If you acidify with a different acid (such as hydrochloric), then regardless of which base you use, you'll want to have an excess of base so that you can distill the lactic acid (ew!) without any excess acid coming over.

Just hypothesizing here, but you might also be able to hydrolyze the polymer by refluxing it in aqueous acid for a while, adding just enough bicarbonate to neutralize the acid that you've added, and then distilling.

Yeah, I did the math and sulfuric is the best option unfortunately. Even compared to buying lactic acid. 24 a gallon and a half at Home Depot, the PLA is waste anyway, and eggshells are a fine source of calcium. less than a cent per gram if I do it that way rather than like a dollar per gram on eBay.
View user's profile View All Posts By User