Any suggestion or procedure for synthesis Rh2(SO4)3 ??

I found reference that mentioned reaction of sulfuric acid with rhodium metal at 400c lead to red rhodium(III) sulfate but this route need special equipments.

This is difficult to make rhodium salt from metal.

Anyone has experience on synthesis of this component?




Chemistry = Chem + is + Try
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6351
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 20-7-2022 at 02:53


What is your source of rhodium?
I presume you are working at a very small scale.
View user's profile View All Posts By User
Waffles SS
Fighter
****




Posts: 998
Registered: 7-12-2009
Member Is Offline


[*] posted on 20-7-2022 at 03:11


Quote: Originally posted by j_sum1  
What is your source of rhodium?
I presume you are working at a very small scale.


My source of Rhodium is metal.

My scale is 5gr and i want to use Rhodium Sulfate for plating


[Edited on 20-7-2022 by Waffles SS]




Chemistry = Chem + is + Try
View user's profile View All Posts By User
paulll
Hazard to Others
***




Posts: 112
Registered: 1-5-2018
Member Is Offline

Mood: It's fine. Really.

[*] posted on 20-7-2022 at 14:41


Could https://patents.google.com/patent/RU2112063C1/en be of use?
View user's profile View All Posts By User
Waffles SS
Fighter
****




Posts: 998
Registered: 7-12-2009
Member Is Offline


[*] posted on 21-7-2022 at 03:27


Quote: Originally posted by paulll  
Could https://patents.google.com/patent/RU2112063C1/en be of use?

Thanks but i am looking for red Rhodium Sulfate(Rh2SO3) not yellow one.




Chemistry = Chem + is + Try
View user's profile View All Posts By User
Rainwater
National Hazard
****




Posts: 964
Registered: 22-12-2021
Member Is Offline

Mood: Break'n glass & kick'n a's

[*] posted on 21-7-2022 at 14:03


It will be slightly reactive with aqua regia. Maybe use your nugget as an anode? I melt and sell mine. $$$

Most of its salts are very toxic with LD under 200mg per kilo




"You can't do that" - challenge accepted
View user's profile View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1247
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 21-7-2022 at 23:18


Rhodium reacts with aqua reagia only at high pressure and temperature.

http://www.ajchem-a.com/article_92164_e9bc6183bdc619dec8940a...

Rhodium is usually dissolved in molten NaHSO4 or KHSO4.
View user's profile View All Posts By User
MidLifeChemist
Hazard to Others
***




Posts: 192
Registered: 4-7-2019
Location: West Coast USA
Member Is Offline

Mood: precipitatory

[*] posted on 10-8-2022 at 14:16


PSA - 5 grams is $2,500 USD worth.
View user's profile View All Posts By User

  Go To Top