Tungsten rod not pure ?


For using as an anode for an electric arc furnace I ordered two W rods of 200mm long x 5mm diameter.
https://www.ebay.com/itm/224180442907
I received them after a week and they indeed appeared like tungsten, felt rather heavy.
Then I checked the density and it appeared to 53g per rod which means 53g/((0.25cm)2*pi*20cm) which means 13.4 g/cm3, well below the real density of W which is 19.3.

Or is it really 'cemented tungsten steel' which means a steel core with W wrapped around it which explains the low density ?

And is this really 99+ % W metal ?

https://www.ebay.com/itm/314087659398
View user's profile View All Posts By User
violet sin
International Hazard
*****




Posts: 1462
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Online

Mood: Good

[*] posted on 24-12-2022 at 12:09


Get a tig welding rod pure W. 3/16" is almost 5mm but they not cheap. I see ~75$ US for 7pc pack?


Cemented Carbide vs Tungsten Steel
https://www.samaterials.com/content/cemented-carbide-vs-tung...

Generally speaking, tungsten steel is smelted by adding tungsten raw materials into molten steel by steelmaking process, and its tungsten content is generally 15-25%
View user's profile View All Posts By User
Chemetix
National Hazard
****




Posts: 374
Registered: 23-9-2016
Location: Oztrayleeyah
Member Is Offline

Mood: Wavering between lucidity and madness

[*] posted on 24-12-2022 at 12:11


The wording 'Tungsten steel round bar rods' is a giveaway....Tungsten steel as in a steel alloy containing tungsten.
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1688
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 24-12-2022 at 13:19


The designation isn't correct , but I think it's safe to assume it's 'K10 Cemented Tungsten Carbide':
https://carbide.ultra-met.com/item/iso-grades/iso-grade-clas...

Basically it's a high strength composite composed of 94% tungsten carbide in a 6% cobalt matrix. You need to look for welding electrodes.

You should also familiarize yourself with the available types:
https://www.thefabricator.com/thewelder/article/consumables/...





We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
metalresearcher
International Hazard
*****




Posts: 729
Registered: 7-9-2010
Member Is Offline

Mood: Reactive

[*] posted on 25-12-2022 at 00:40


Quote:
You need to look for welding electrodes.

Something like this from Amazon ?
https://www.amazon.com/s?k=tungsten+electrode&crid=1QIKZ...
View user's profile View All Posts By User
violet sin
International Hazard
*****




Posts: 1462
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Online

Mood: Good

[*] posted on 25-12-2022 at 01:10


Green for pure tungsten. I'm a fan of orange, 4% thoriated for my collection of radioactive oddities collection. There are different colors for a quick reference to composition. In the TIG environment, some run better AC or DC and react to frequency diff. I'm a newbie to TIG, have the machine but still looking for n argon bottle I can afford.

Here maybe try this
3/16" pure tungsten ~75$ US
https://www.amazon.com/Pure-Welding-Tungsten-Electrodes-Gree...
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1688
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 25-12-2022 at 01:15


Yup, that's the right stuff.



We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
Mateo_swe
National Hazard
****




Posts: 493
Registered: 24-8-2019
Location: Within EU
Member Is Offline


[*] posted on 30-12-2022 at 14:29


The second ebay link in OPs post states its pure tungsten rod 99.99%
But they are only 100mm long and a 5mm diameter is 12.89 GBP or about 14,5 Euros.
Seems they have lots of different thickness, 2 to 15mm diameter.
The TIG tungsten rods i think is pure tungsten also but there is different variants so choose the pure tungsten one.

A 10Liter 100% Argon 200bar bottle in Europe is about 150 Euros on Ebay (one time use bottle).
You could buy a refillable bottle and then the refills are cheap but the refillable bottle is expensive.
View user's profile View All Posts By User
Admagistr
National Hazard
****




Posts: 289
Registered: 4-11-2021
Location: Central Europe
Member Is Offline

Mood: The dreaming alchemist

[*] posted on 30-12-2022 at 14:35


Quote: Originally posted by Mateo_swe  
The second ebay link in OPs post states its pure tungsten rod 99.99%
But they are only 100mm long and a 5mm diameter is 12.89 GBP or about 14,5 Euros.
Seems they have lots of different thickness, 2 to 15mm diameter.
The TIG tungsten rods i think is pure tungsten also but there is different variants so choose the pure tungsten one.

A 10Liter 100% Argon 200bar bottle in Europe is about 150 Euros on Ebay (one time use bottle).
You could buy a refillable bottle and then the refills are cheap but the refillable bottle is expensive.


It's the one marked in green! That's pure tungsten!
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3469
Registered: 8-2-2015
Location: UK
Member Is Offline


[*] posted on 31-12-2022 at 04:38


I used tungsten rods like the ones in the second link for spark gap tesla coils,
the erosion was so negligible that I believe they were/are pure tungsten.




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
Fery
International Hazard
*****




Posts: 951
Registered: 27-8-2019
Location: Czechoslovakia
Member Is Offline


[*] posted on 1-1-2023 at 09:22


Just visit welding shop personally and tell them that you want pure tungsten electrodes. In my country they are 99,8% pure W (green electrodes). I bought also the mentioned orange electrodes which contain 4% ThO2 - the e-shop even contacted me that they found few more orange electrodes, whether I do not want to buy them too (because I bought all they had in their e-shop system), that nobody uses them today for welding due to toxicity so they gave me a discount (wanted to get rid of them). Owning this form of Th is legal in my country.
View user's profile Visit user's homepage View All Posts By User
Texium
Administrator
Thread Moved
14-9-2023 at 11:44

  Go To Top