PET Solvent


Are there any good solvents for PET at near room temperature? I've used boiling diethylene gylcol (nearly 200 C), but am looking for something that will work on the bench top.
View user's profile View All Posts By User
Bot0nist
International Hazard
*****




Posts: 1559
Registered: 15-2-2011
Location: Right behind you.
Member Is Offline

Mood: Streching my cotyledons.

[*] posted on 18-4-2011 at 07:40


For polyethylene terephthalate;

Phenol, chlorophenol, nitrobenzene and dimethyl sulphoxide. BHET maybe.