Author: Subject: Gold salts synthesis, and other precious metal salts.
Megamarko94
Hazard to Self
**




Posts: 68
Registered: 31-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 26-5-2011 at 14:56
Gold salts synthesis, and other precious metal salts.


if you have any gold salt synthesis pls. post it...or any other precious metal salt.....
View user's profile View All Posts By User
LanthanumK
Hazard to Others
***




Posts: 298
Registered: 20-5-2011
Location: New Jersey
Member Is Offline

Mood: No Mood

[*] posted on 26-5-2011 at 16:33


The dissolution of gold and palladium in aqua regia is well known. Platinum also dissolves. All of these form precious metal compounds, although I am not sure whether they are known as salts.
View user's profile Visit user's homepage View All Posts By User
cyanureeves
National Hazard
****




Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline

Mood: No Mood

[*] posted on 26-5-2011 at 17:05


silver nitrate is simply made by dissolving silver in nitric acid. sterling in nitric acid will make a contaminated silver nitrate solution that can be turned into silver chloride by adding table salt to it. or use a pure silver nitrate solution if you have pure silver.electrolyzing gold in potassium cyanate will make a gold solution but i've never went as far as evaporating the solution to see what the salt will look like. if you evaporate gold chloride it will turn syrupy and i dont see why it wouldnt make a salt if further dried.to make the cyanate or cyanide synthesis go to the preparation of cyanide thread. that is as preciously as i've gone. i've never even touched platinum.
View user's profile View All Posts By User
Neil
National Hazard
****




Posts: 556
Registered: 19-3-2008
Member Is Offline

Mood: No Mood

[*] posted on 27-5-2011 at 08:58


The Chemistry of Gold
M. Concepción Gimeno

http://www.wiley-vch.de/books/sample/3527320296_c01.pdf