I just accidentally poured some KBH4/NaOH solution into a solution of Nickle (II) sulphate, then the green precipitate appeared as expected, but then after a few seconds, the precipitate turned black, with Hydrogen bubbling out from solution.

So is the grey-black powder Nickel metal?
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5102
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 4-12-2011 at 03:30


Could be nickel boride which gets a mention here

http://en.wikipedia.org/wiki/Nickel(II)_chloride
View user's profile View All Posts By User
KrysHalide
Harmless
*




Posts: 19
Registered: 29-11-2011
Location: France
Member Is Offline

Mood: No Mood

[*] posted on 4-12-2011 at 04:31


Definitevly Ni Boride!! That's a method of choice for it's preparation. It decomposes the remaining BH4- into H2...



Never regret thy fall,
O Icarus of the fearless flight
For the greatest tragedy of them all
Is never to feel the burning light.

Oscar Wilde
View user's profile View All Posts By User
LHcheM
Harmless
*




Posts: 37
Registered: 20-2-2011
Member Is Offline

Mood: No Mood

[*] posted on 4-12-2011 at 05:18


Oh I never thought of that! Nickel Boride! Thanks!!!

A useful reagent for Organic reactions :)