ONeill
Harmless
Posts: 5
Registered: 7-10-2012
Member Is Offline
Mood: No Mood
|
|
Cu from Cu(I)Cl
Hello folks,
I´m trying to get elemental copper from Cu(I)Cl. I have tried thermal decomposition in inert gas with temperatures between 200 an 600 °C, but the
result was just a grey powder that decomposes in air within some hours to a green solid. At higher temperatures the salt just evaporates.
In the next days I will try to decompose the copper chloride in degassed water to get Cu(II) and Cu.
Any new ideas, maybe a reducing agent like NaBH4?
Thanks for your comments.
Cheers ONeill
|
|
|
Mumbles
Hazard to Others
 
Posts: 436
Registered: 12-3-2003
Location: US
Member Is Offline
Mood: Procrastinating
|
|
Your best best is probably to convert to a water soluble form, and reduce it with aluminum, iron, or zinc. Oxidizing it to the generally much more
soluble copper (II) is one possibility, followed by reduction. Copper (I) Chloride can be made soluble by a variety of things. Dissolving it in HCl
or another halide source would probably be my first attempt as far as this goes.
If you want to reduce it with heat, you might try to run the thermal decomposition in a hydrogen stream. This works for Copper (I) oxide, and several
other chlorides. I just don't know off hand if it definitely works for copper (I) chloride though.
[Edited on 10-7-2012 by Mumbles]
|
|
|
kristofvagyok
National Hazard
  
Posts: 659
Registered: 6-4-2012
Location: Europe
Member Is Offline
Mood: No Mood
|
|
Have tried thermite reaction? CuCl could be also converted to Cu with Al and it could be washed with cc HCl to remove impuries.
Or heat it up in a H2 steam... I think that it will also work... It worked for me with CuO and Cu2O.
I have a blog where I post my pictures from my work: http://labphoto.tumblr.com/
-Pictures from chemistry, check it out(:
"You can’t become a chemist and expect to live forever."
|
|
|
Hexavalent
International Hazard
   
Posts: 1564
Registered: 29-12-2011
Location: Wales, UK
Member Is Offline
Mood: Pericyclic
|
|
Yesterday I prepared some copper powder by the reduction of copper (II) sulfate with ascorbic acid (using dilute ammonia solution to control pH and
'coagulate' the fine powder into larger particles). The reduction is more favourable than formation of a complex so the process works rather well.
"Success is going from failure to failure without loss of enthusiasm." Winston Churchill
|
|
|
blogfast25
International Hazard
   
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Copper is so easy to make it's not worth sacrificing an expensive (and unstable) compound like CuCl (I) on it.
'Themiting' chlorides doesn't work. Generally speaking AlCl3 has far too low Heat of Formation, it is also very volatile (sublimes). Generally
speaking reducing chlorides pyrometallurgically requires closed reactors to confine the volatile chlorides (see e.g. Kroll Process)
[Edited on 8-10-2012 by blogfast25]
|
|
|
ONeill
Harmless
Posts: 5
Registered: 7-10-2012
Member Is Offline
Mood: No Mood
|
|
Hello guys,
thank you for you answers!
Quote: Originally posted by Mumbles  | | Copper (I) Chloride can be made soluble by a variety of things. Dissolving it in HCl or another halide source would probably be my first attempt as
far as this goes. |
I will try to make a solution with typical solvents, any idea what works good? HCl and ammonia should work good (building of complexes), but I woul
prefer a neutral solvent.
Quote: Originally posted by Mumbles  | | If you want to reduce it with heat, you might try to run the thermal decomposition in a hydrogen stream. This works for Copper (I) oxide, and several
other chlorides. I just don't know off hand if it definitely works for copper (I) chloride though. [Edited on 10-7-2012 by Mumbles]
|
I´m shure that this would work, but I would like to find an alternative for hydrogen as reducing agent.
Shure this would work but I would prefer to use a homogenous solution as reducing agent. Thank you.
Quote: Originally posted by Hexavalent  | | Yesterday I prepared some copper powder by the reduction of copper (II) sulfate with ascorbic acid (using dilute ammonia solution to control pH and
'coagulate' the fine powder into larger particles). The reduction is more favourable than formation of a complex so the process works rather well.
|
This could be a good alternative, thank you.
I´ve got a lot of Cu(I)Cl and If I don´t use it it will be thrown away 
Thanks again for your answers.
Cheers ONeill
|
|
|