Aluminum magnesium ratio


I have been looking around at different incendiary bullets and most of them use a compound made of barium nitrate and a alumnium and magnesium alloy does anyone know what the alloys ratio of magnesium to aluminum is or have any other info on it?



View user's profile View All Posts By User
DubaiAmateurRocketry
National Hazard
****




Posts: 841
Registered: 10-5-2013
Location: LA, CA, USA
Member Is Offline

Mood: In research

[*] posted on 8-12-2013 at 17:09


its called magnalium powder.
wiki link
http://en.wikipedia.org/wiki/Magnalium

for pyrotech its usually Mg·Al, so around 50:50