Serious descaling
Gents, there is a wonderful invention called the 'zojirushi'. It sits quietly next to the coffee pot, keeping water hot for whenever I need it. It's
a wonderful, wonderful thing.
But, it's got a serious scale problem. Scale sticks like a barnacle to the side until it breaks off in huge chunks that floats around. It gets
nasty.
My normal solution to this would be vinegar, and attack with a rough ss scouring pad. But, this particular model has a polymer (teflon??) lining, and
I don't want to scratch that up. It's too soft even for scotchbrite.
I need a chemical solution, one that is unlikely to fubar the pump seals, that can be reliably flushed from the system so I don't poisen us, and that
will work. My first instinct was dump a shot glass of concentrated H2SO4 or HCL in there.
But I thought I'd ask here, first.
|
|
ScienceSquirrel
International Hazard
   
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
Most commercial descalers use citric acid.
Lactic, sulphamic and formic acids are also used.
Zojirushi have a product that is based on citric acid and the machine has a nifty cleaning cycle as well so put your sulphuric acid away!
http://www.zojirushi.com/products/cdk
|
|
plante1999
International Hazard
   
Posts: 1936
Registered: 27-12-2010
Member Is Offline
Mood: Mad as a hatter
|
|
I think there is a product in north america called CLR that supposedly works.
I never asked for this.
|
|
Pyro
International Hazard
   
Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline
Mood: No Mood
|
|
don't use H2SO4, that makes CaSO4, plaster of Paris. use HCl, but diluted.
the wisest course of action however, is to buy a descaling kit. that way there is no risk of damaging your thing.
all above information is intellectual property of Pyro. 
|
|
Nickdul
Hazard to Self

Posts: 96
Registered: 13-2-2012
Location: Bulgaria
Member Is Offline
Mood: No Mood
|
|
A product I use commonly has these listed on the MSDS:
Citric Acid: <60%
Tartaric Acid <35%
EDTA <5%
The packaging is 250g and is supposed to be diluted with 750 to 1000ml with water. You can make out the percentages and try it.
|
|