I was board so I stated massing around with some wax I had a sheet of that I wormed up a little so it was bendable so I made a funnel and even some Test-tube by dipping a Test-tube in molten wax and let it cool I then removed the wax by adding boiling water in the Test-tube the wax slid off easily than had a nice wax Test-tube I could also make beakers it seems to be a nice cheap way to get Test-tube and such but they would be limited to experiments

Sorry for the post I am still board




View user's profile Visit user's homepage View All Posts By User
thalium
Hazard to Others
***




Posts: 123
Registered: 2-11-2004
Location: Bottom of Hell
Member Is Offline

Mood: :D

[*] posted on 2-1-2005 at 03:52


Nice..but I don't think they'll resist



I don\'t believe in ghosts but they believe in me


Hell was full so I came back..
View user's profile Visit user's homepage View All Posts By User
garage chemist
chemical wizard
*****




Posts: 1803
Registered: 16-8-2004
Location: Germany
Member Is Offline

Mood: No Mood

[*] posted on 2-1-2005 at 04:58


But sure they'll resist Hydrofluoric acid!

But they can't be warmed, because they would melt.

It is also possible to coat a test tube/beaker/flask with paraffin on the inside (very thin coating, a fraction of a millimeter thick) and these can also be used for HF experiments.
Would the coating stay intact if the glass was heated? If yes, we could immerse our distilling equipment and flasks in molten paraffin and could then use them for making HF!
View user's profile View All Posts By User
chemoleo
Biochemicus Energeticus
*****




Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline

Mood: crystalline

[*] posted on 2-1-2005 at 05:13


Why not just using polyethylene/propylene tubing/flasks etc?
If wax is resistent, then PE/PP surely is!




Never Stop to Begin, and Never Begin to Stop...
Tolerance is good. But not with the intolerant! (Wilhelm Busch)
View user's profile View All Posts By User
kclo4
National Hazard
****




Posts: 916
Registered: 11-12-2004
Location:
Member Is Offline

Mood: No Mood

[*] posted on 2-1-2005 at 12:52


You could also do it with polyethylene/propylene but you might have a problem getting it off as for using wax it is cheaper and is reparability you just have to melt it again :)



View user's profile Visit user's homepage View All Posts By User
neutrino
International Hazard
*****




Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline

Mood: oscillating

[*] posted on 2-1-2005 at 14:24


Play around with molten plastic and you’ll be begging to use wax. Because of the wax’s low melting point, you can shape it with your hands. No messy molds to deal with.
View user's profile View All Posts By User
kryss
Hazard to Self
**




Posts: 77
Registered: 11-7-2003
Location: N Ireland
Member Is Offline

Mood: No Mood

[*] posted on 2-1-2005 at 16:35


As well as using ordinary wax you could try wrapping in glass fibre or using as a mould for resin items.
View user's profile View All Posts By User
evilgecko
Harmless
*




Posts: 36
Registered: 2-1-2005
Member Is Offline

Mood: Decomposing

[*] posted on 3-1-2005 at 14:54