Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Things to do with Nickel
Fleaker
International Hazard
*****




Posts: 1253
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 30-7-2005 at 19:23
Things to do with Nickel


Just purchased 500g of very decent quality nickel metal (4N5) 2cm by 2cm by .5cm thick. Having done so on an impulse, I'm now quite puzzled as to what to do with it. Do any of you think it would be feasible to make Raney nickel catalyst? While I'm melting it I should probably cast some thin plates for anode duty too.

Do nickel/chromium crucibles have good chemical resistance?


Thanks for any insight/ideas.
View user's profile View All Posts By User
BromicAcid
International Hazard
*****




Posts: 3313
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline

Mood: Rock n' Roll

[*] posted on 30-7-2005 at 22:58


Nickel is fun stuff to have around. Nickel crucibles are great for their chemical resistance, noteably to bases. Nickel electrodes are also great to have around. As to making Raney Nickel, that is just one of my someday fun projects. I precipitated nickel oxylate from nickel chloride and decomposed it and I intend to heat that with aluminum powder to get the alloy which can then be treated with aqueous base. The reaction betwen nickel and aluminum powder described as very vigorous by some members of this forum.

Also there are fun chemical experiments to do with it, such as attempting to acheive some of its higher oxidation states, I made a post on this awhile back and put up the relevent data on some of the information I found on high oxidation state nickel. Of course don't forget its possibilites for catalysis of other reactions, and also making lab ware with it, I bought mine in the form of rods and dissolved them by using them as anodes in electrolysis leaving sharp points at the ends, these have become very utilitarian in my lab, their chemical resistance combined with their strength making them great to use.

I could go on and on about nickel but there really is a lot to do with it, so have fun!




Shamelessly plugging my attempts at writing fiction: http://www.robvincent.org
View user's profile Visit user's homepage View All Posts By User
JohnWW
International Hazard
*****




Posts: 2849
Registered: 27-7-2004
Location: New Zealand
Member Is Offline

Mood: No Mood

[*] posted on 31-7-2005 at 00:59


Oh yes. I am sure that nickel could be used for many things for which the much more expensive palladium and platinum are used. As well as crucibles and implements requiring corrosion resistance, it can substitute for Pd and Pt for many applications as an heterogenous catalyst, particularly where the absorption of hydrogen is required for hydrogenation or catalytic reduction. However, for this application it would not be as efficient as palladium or platinum.
View user's profile View All Posts By User
Fleaker
International Hazard
*****




Posts: 1253
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 31-7-2005 at 09:25


It is true that nickel catalysts (Raney or Urushibara) are not quite as active as palladium on carbon or platinum but when one considers their price and relative easy of preparation, they become more attractive. I have a friend who is/was doing a college study of the effectiveness of Urushibara catalysts in hydrogenation and had some interesting results.

After reading Bromic's thread on electrochemical sodium (the one with the NaOH) I might use some of this nickel for making some large electrodes. I wonder how malleable nickel is? Do you think I could flatten it out on anvil or would it shatter?
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 31-7-2005 at 09:50


Should be about as ductile as copper. If nothing else it can be annealed or hot forged as copper or (pure) iron, both of which it closely resembles, chemically and metallurgically.

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
S.C. Wack
bibliomaster
*****




Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline

Mood: Enhanced

[*] posted on 31-7-2005 at 11:36
Raney alloy


THE SKIP THIS, ITS OFF-TOPIC PART:
I was having a little discussion with ning at WD some months ago, causing me to separate a pile of precursor to/prep/uses of substituted cinnamic acid articles from a much larger pile, and look through them again. He posted a couple of oxidation of subs. cinnamic acid articles that I hadn't seen before, as I was more interested in reduction. I had earlier lost interest in using typical hydrogenation cats. or that much Na to give the saturated cpd., then using an inorganic chloride to give the amide with NH4OH.

The point is, just after ning wrapped up and there was nothing more to say, and it was a ketone thread anyways, I noticed that one of these photocopies, JACS 62, 161 (1940) said: "a-Methyl-2,5-dimethoxyhydrocinnamide.-The amide was obtained by heating the corresponding hydrocinnamic acid (above) in a stream of ammonia at 220-230° for two hours. Recrystallized from benzene it forms a finely crystalline powder melting at 99°." That was one of the more detailed steps in the article. OK, maybe urea could also give the amide. But there is still the hydrogenation, to get to the a-methylphenylpropionic acid.

THE ON-TOPIC PART:
Then I noticed in JOC 22, 33 (1957): "DL-a-Methylhydrocinnamic acid (I) mas prepared in 95% yield by treating 30 g. of a-methylcinnamic acid and 99.8 g. of sodium hydroxide in 900 ml. of water with 90 g. of Raney nickel-aluminum alloy at 90°. The cooled filtrate and washings were stirred into 720 ml. of concd. hydrochloric acid and about 700 g. of ice and extracted with ether (600 + 300 + 300 ml.). The ether extracts were washed with 2 N hydrochloric acid and with sodium chloride solution, dried, and evaporated. The distilled acid (b.p. 148-149'/9 mm., 116.5'/0.5 mm.) solidified on chilling; m.p. 36-37°; yield 28.9 g. (95%). A sample crystallized from pentane in colorless prisms, m.p. 36.6-37.5° (lit. m.p. 37°)"

Nifty. The hydrogen from the dissolving Al (or additional aluminum) provides all you need, without pressure.

This led me to JOC 9, 175 (1944), which led me to 7, 587 (1942), 9, 1 (1944), and IEC Anal 15, 576 (1943). Wow. Following up led me to JOC 10, 233 (1945) and Chem Rev 89, 459 (1989).

In short, in alkali OH it reduces alkenoic acids to alkanoic, reduces or doesn't aryl ethers or unsaturated rings, quantitatively reduces halogen functions (leaves them alone in organic acid), reduces the usual N-functions to amines like other hydrogenation cats. do (nitriles to aldehydes in organic acid), ketones to alcohols or alkanes, or to amines when ammonia is used. And much more. There is a lot of unexplored/unpublished territory, esp. in the reductive amination, nitro-whatever, and co-solvent dept. No doubt much private research has/will be done, there is a host of obvious new substrates.

axehandle has all of my Chem Revs, BTW. Here are the mentioned alloy articles, as this does not seem to be as widely known as it should be.
View user's profile Visit user's homepage View All Posts By User
S.C. Wack
bibliomaster
*****




Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline

Mood: Enhanced

[*] posted on 2-8-2005 at 19:14


The above reductions by Raney alloy collection of articles was uploaded too soon, I have three more, although no one else gives a shit/was unaware. They are JOC 27, 3873 (1962), Chem. Commun. 514 (2003), and JCS 531, (1966). Some likely more interesting articles are unavailable to me.
View user's profile Visit user's homepage View All Posts By User
Fleaker
International Hazard
*****




Posts: 1253
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 2-8-2005 at 20:15


Thanks very much for making those available to me, I appreciate it and I'll take a look asap.
View user's profile View All Posts By User
enima
Hazard to Self
**




Posts: 98
Registered: 1-12-2004
Member Is Offline

Mood: No Mood

[*] posted on 2-8-2005 at 21:40


Raney alloy preparation.

Does anyone have information about making the alloy. I know its suppose to have 50/50 Ni-Al. Would one use the metal powders of each, mix them together and slowly heat until they both become molten in a crucible?

Will either powder ignite during the heating process? A butane burner could be useful as it reaches a nice temp of 1300C.
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 3-8-2005 at 00:40


Aren't AlNi intermetallics exothermic? Powder could be quite interesting then, though not particularly useful!

The best way to prepare would be a vacuum or inert gas furnace capable of melting nickel, next to that you need a flux resistant to aluminum which means no silicate flux like nickel would prefer. Fluorite may be able to do this, as IIRC its melting point is around there. For sure it forms low eutectics will all sorts of things, but I don't know how many of those are aluminum-compatible. Oh, and use a good solid crucible also resistant to aluminum and as resistant to fluorospar as possible (now that's a toughie).

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
Fleaker
International Hazard
*****




Posts: 1253
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 3-8-2005 at 17:46


I was going to do it in a fused quartz crucible (chemical compatibility there?) which would take the temperature well. I don't mixing the powders and heating is necessary. I would probably melt the nickel and add the apporpriate mass of Al.

Oh by the way, took one of the nickel pieces to the anvil, and it's remarkably resilient to hammer strokes: no deformation whatsoever. I should mention that it's very thick. I didn't have time to heat it however.
View user's profile View All Posts By User
BromicAcid
International Hazard
*****




Posts: 3313
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline

Mood: Rock n' Roll

[*] posted on 3-8-2005 at 18:26


Yes 12AX7, the reaction is a self-sustaining exotherm between the metals, not only has this been described by other members of this forum, but that is what I ment by the two powders undergoing an 'very vigorous' reaction together.



Shamelessly plugging my attempts at writing fiction: http://www.robvincent.org
View user's profile Visit user's homepage View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 4-8-2005 at 05:38


Say, is the powder like thermite, flash or what? :o

Fused quartz might do it, but Al + SiO2 ~= Si + Al2O3 so it wouldn't really be preferrable if you want purity. I'd use sintered or fused alumina or magnesia, whichever's cheaper..

BTW here's some typical data on nickel. Pretty ferric in characteristics, lack of transformation temperature and low curie point aside. http://www.matweb.com/search/SpecificMaterial.asp?bassnum=NL...

Tim

[Edited on 8-4-2005 by 12AX7]




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
Fleaker
International Hazard
*****




Posts: 1253
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 5-8-2005 at 12:29


I forgot about that (ref: Al+ SiO2). Alumina is cheaper.
View user's profile View All Posts By User

  Go To Top