Morgan
International Hazard
*****




Posts: 1560
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 27-12-2017 at 11:15
Pink Quartz


So I ordered some quartz tubing, this listing on eBay - 2pcs Quartz Glass Capillary Tube Outer Diameter 16mm ID 12mm Length 150mm #A4R3 from fanty_store and got something that has a pink tint to it. It's obvious at the ends but even the tubing itself you can tell it has some sort of faint impurity in it. And the outsides had minor scuff marks and something weird going on if you hold it up to the light.

DSC_0018.JPG - 146kBDSC_0014.JPG - 154kBDSC_0010 (2).JPG - 193kBDSC_0015 (1).JPG - 134kB
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 4902
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 27-12-2017 at 11:34


Could be they started with this
https://en.wikipedia.org/wiki/Quartz#Rose_quartz
View user's profile View All Posts By User
Chemetix
National Hazard
****




Posts: 368
Registered: 23-9-2016
Location: Oztrayleeyah
Member Is Offline

Mood: Wavering between lucidity and madness

[*] posted on 27-12-2017 at 12:57


Your link to fanty_store is hard to pick up do you have a direct link ? Looks like a perfect example of Chinese manufacturing QC.
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1560
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 27-12-2017 at 13:57


Here's all the sizes they offer. I was just wondering what the trace element(s) are in the tubing.
https://www.ebay.com/sch/i.html?_from=R40&_trksid=m570.l...
View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 27-12-2017 at 17:20


Quote: Originally posted by Morgan  
Here's all the sizes they offer. I was just wondering what the trace element(s) are in the tubing.
https://www.ebay.com/sch/i.html?_from=R40&_trksid=m570.l...


According to Wikipedia, your main suspects would be Ti, Fe, and/or Mn.

Personally, I think it looks rather nice, but I suppose that doesn't matter if the glass turns out to be weaker or less chemically resistant somehow.




Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
violet sin
International Hazard
*****




Posts: 1388
Registered: 2-9-2012
Location: Back yard staring at stars
Member Is Offline

Mood: Good

[*] posted on 27-12-2017 at 17:51


I purchased a couple 4" x ~0.5" quartz tube a while ago, it was orange and specifically to block UV. Some aquarium thing I believe. Most the time you want to pass the UV, but I guess some times that is not the plan.

"UV quartz flow tube 70mm" in health and beauty section.

The seller is no longer registered and a product name search turned up nothing. It was back in 2015





View user's profile View All Posts By User
RogueRose
International Hazard
*****




Posts: 1576
Registered: 16-6-2014
Member Is Offline


[*] posted on 27-12-2017 at 19:33


I would suspect it is still the 99%+ purity of what most quartz glassware is and those "contaminates" are from the natural quartz color and I'd doubt that it would hurt the tubes. I've seen pink quarts MUCH darker than that, though it was in its natural state so it wouldn't be as clear as having been melted and moulded. I'd guess that these are alright as far as the color issue, but those markings when held to the light, IDK what that is.
View user's profile View All Posts By User
KalleMP
Harmless
*




Posts: 13
Registered: 5-12-2016
Member Is Offline

Mood: No Mood

[*] posted on 27-3-2018 at 12:32


Scuff marks or striations are common, almost a feature of fused quarts tubing.

Any glass worker will tell you that the stuff is very different from regular glasses and as a single compound it has a much narrower plastic temperature range, it melts suddenly and so has to be extruded under higher pressure below the melting point through dies to make tubing and does not flow smooth after extrusion like glass tubing will.

Rose quarts is pretty and the amount of contaminants that colour gemstones are usually very small. The raw material has been purified by crystallisation after all.

Purple quarts though is I think a result of other contaminants being irradiated.

Then there is the thing with small Radiohalos due to alpha radiation at the ends of microscopic cracks in some minerals.

https://en.wikipedia.org/wiki/Radiohalo
View user's profile View All Posts By User
diddi
International Hazard
*****




Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline

Mood: Fluorescent

[*] posted on 27-3-2018 at 14:06


great for mineral collectors and chemists alike!



Beginning construction of periodic table display
View user's profile View All Posts By User
Radium212
Hazard to Self
**




Posts: 85
Registered: 26-6-2017
Member Is Offline

Mood: Pyrophoric.

[*] posted on 28-3-2018 at 02:49


I've heard that Fe or Ni will do that. Never seen it though.
View user's profile View All Posts By User
DrP
International Hazard
*****




Posts: 625
Registered: 28-9-2005
Member Is Offline

Mood: exothermic

[*] posted on 28-3-2018 at 05:06


I have some large chunks of rose quartz. It is an attractive crystal.