D.I.Y. Silicone Stoppers/Bungs ?


Yet again I have a partially used, solid, unusable cartridge of silicone sealant :(
This time I opened it up:

SillyCone.jpg - 2.1MB

The long tapered part can be cut into a series of small stoppers,
the large round rod may have a use ?
BUT
For some uses such as adapting ground glass to other materials it may not be too difficult to cast a re-usable stopper using fresh silicone rubber.
D.I.Y. could be cheaper and more versatile.

Just thought I'd air the idea here in case it is of use to anyone.

View user's profile View All Posts By User
j_sum1
Super Moderator
*******




Posts: 3884
Registered: 4-10-2014
Location: Oz
Member Is Offline

Mood: Metastable, and that's good enough.

[*] posted on 12-7-2018 at 02:44


I have three or four of these at present. Different products. I deliberately left them open after the last couple of jobs to see if I could get something useful. I have seen them converted to stoppers on a yt video - on a lathe I think. But I can't remember where.
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 1806
Registered: 8-2-2015
Location: England
Member Is Offline


[*] posted on 12-7-2018 at 03:13


I just cut a length of the large rod as it fits my 2l Erlenmeyer almost perfectly :D
the Erlenmeyer that I just last month bought a white rubber stopper for :P



Irrelevant:
I won the flask via eBay in April for £1.00, listed as
"60 corks from wine bottles and champagne bottles in decorative glass flask ",
Pyrex brand, even the base is hardly scratched :D

From the same seller I also won
5x 25ml volumetric flasks with ground glass stoppers for £1.00
and
2x 250ml glass bottles with ground glass stoppers for £2.60
- that my wife thought were too cute for chemistry so they are now in the kitchen :(
so I even got combined postage for £7.50
... a good hobby day

[Edited on 12-7-2018 by Sulaiman]
View user's profile View All Posts By User
zed
International Hazard
*****




Posts: 1618
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline

Mood: Semi-repentant Sith Lord

[*] posted on 12-7-2018 at 15:28


I have applied this type of Silicone sealant, and the solvent in it, as I remember by smell, is Glacial Acetic acid.

So, it has good chemical resistance, but perhaps not to everything.