I picked it up out of the university trash; I think it might have been part of a large aquarium heater. It's ~38", OD 1", thickness ~1/8", and closed
off on one end like a long, wide test tube. It's not obvious what kind of glass it is, but if my guess about its origin is right I'd expect it to have
reasonable heat stability.
So far it's an acquisition in search of a purpose. I haven't come up with an application that would really be suited to it's nature, other than maybe
some sort of gas-phase reaction.
Any ideas?
[Edited on 28-8-2018 by mayko]
al-khemie is not a terrorist organization
"Chemicals, chemicals... I need chemicals!" - George Hayduke
"Wubbalubba dub-dub!" - Rick Sanchez
|
|
SWIM
International Hazard
   
Posts: 970
Registered: 3-9-2017
Member Is Offline
|
|
If it's from a water purifier, it might be quartz!
Don't know an easy way to tell the difference, but if it is, it's one mighty refractory tube, and not a cheap item to buy.
|
|
Foeskes
Hazard to Others
 
Posts: 156
Registered: 25-2-2017
Member Is Offline
Mood: No Mood
|
|
Tube furnace?
|
|
MrHomeScientist
International Hazard
   
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
You can distinguish quartz from other glass by its ability to transmit UV light. Get a black light and something fluorescent, put the tube on top of
the fluorescent object, and see if it glows when the light is shined through the glass. I did this in my video on burning diamonds.
It also sounds like a candidate for the barking dog reaction, but it might be a little narrow. You also run the risk of shattering the closed end with
the pressure wave! I do that demonstration in a regular glass tube about that length and thickness, but with an OD more like 2". It's also open at
both ends and sealed with rubber stoppers, so if too much pressure develops it will just pop those out rather than break the glass.
[Edited on 8-28-2018 by MrHomeScientist]
|
|
Heptylene
National Hazard
  
Posts: 319
Registered: 22-10-2016
Member Is Offline
Mood: No Mood
|
|
If it is not quartz, it could make a nice starting point for large ampoules of chlorine, bromine etc. for an element collection.
If its quartz you can cut it but you won't be able to fuse it or bend it without an oxygen/propane torch or similar. That's another way to test for
quartz btw: if it looks like glass but you can't melt it, then its probably quartz.
|
|
Ubya
International Hazard
   
Posts: 1213
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
Quote: Originally posted by Heptylene  | If it is not quartz, it could make a nice starting point for large ampoules of chlorine, bromine etc. for an element collection.
If its quartz you can cut it but you won't be able to fuse it or bend it without an oxygen/propane torch or similar. That's another way to test for
quartz btw: if it looks like glass but you can't melt it, then its probably quartz. |
quartz when strongly heated is white, while borosilicate or soda lime glass will color the flame yellow
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
If you are looking for chemicals check this out: [For Sale]300 chemicals (rare & unusual)
---------------------------------------------------------------------
|
|
Deathunter88
National Hazard
  
Posts: 494
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline
Mood: No Mood
|
|
Easiest test for quartz that I know: heat a small part of it until it is really got (>300 degrees C), then plunge into cold water. If it's quartz,
nothing will happen, if it's not, then it will shatter into a thousand pieces.
|
|
JJay
International Hazard
   
Posts: 3440
Registered: 15-10-2015
Member Is Offline
|
|
That will work for detecting quartz all right. I've personally performed that test, first heating the quartz until it was glowing red then plunging it
into a bucket of water. The water will boil, but quartz will survive the treatment every time with 0 damage. Of course, lesser glass might not even
survive the blowtorch.
|
|