Electrical Furnace Contruction - My design and implementation
[quote][i]Originally posted by Cyrus[/i]
I don't understand the irritation in your response. ...
27-7-2004 at 13:27
by: Nevermore
Electrical Furnace Contruction - My design and implementation
hello, pure porcelain and thin should rexist up to molten al temp..a mug is not good for that, is no ...
26-7-2004 at 03:21
by: Nevermore
Silver "does not arc"
i don't completely agree with that, arcing depends mainly on the current and voltage of the two ...
25-7-2004 at 01:35
by: Nevermore
Electrical Furnace Contruction - My design and implementation
[quote][i]Originally posted by Cyrus[/i]
How did the fire kill a crow? Do you mean a crow as in a ...
23-7-2004 at 13:14
by: Nevermore
Electrical Furnace Contruction - My design and implementation
ok here it is the design circuit, on the left you should put the power supply, DC from 12 to 30V at ...
23-7-2004 at 13:12
by: Nevermore
Any erythritol (alchol) synthesis?
[quote][i]Originally posted by kazaa81[/i]
Ok, supposed that erythritol is accepted as sugar substi ...
22-7-2004 at 14:45
by: Nevermore
Electrical Furnace Contruction - My design and implementation
[quote][i]Originally posted by chemoleo[/i]
Are you talking about an induction furnace? I read some ...
22-7-2004 at 10:58
by: Nevermore
peak oil
in my personal opinion we should have enuf oil for 40-50 years more, then it will start to be short. ...
22-7-2004 at 03:50
by: Nevermore
email from idiot
well i got a few messages on aim by a boy that found me on this website, keeps asking me about how t ...
21-7-2004 at 15:32
by: Nevermore
Electrical Furnace Contruction - My design and implementation
[quote][i]Originally posted by axehandle[/i]
At room temperature, at it's maximum allowed work ...
21-7-2004 at 15:29
by: Nevermore
Aluminum chloride
unionised, probably cloric is european, astringent directly derives from latin, is a word used as it ...
21-7-2004 at 15:24
by: Nevermore
U-238 fission
if i remember good is somewhat small, like a couple barn, less than 20 barn for sure for energy arou ...
21-7-2004 at 15:21
by: Nevermore
Degreaser
i found out that NaOH and Na2CO3 work way better when they are together..
i don't know why..
21-7-2004 at 15:14
by: Nevermore
Nitrogen cylinder, welding experience required?
Nitrogen is not friendly with welding since it creates very fragile nitrures during the time the mix ...
21-7-2004 at 15:13
by: Nevermore
Erythritol synth. via bacterias?
moniliella is not a fungus but a yeast, however even Trichosporonoides megachiliensis should be able ...
21-7-2004 at 15:07
by: Nevermore
Paralyzing Substance
[quote][i]Originally posted by hornek[/i]
As I know, the paralyzing staff using in zoo's for p ...
21-7-2004 at 15:04
by: Nevermore
Putrescine & Co.
what about butyric then?
19-7-2004 at 02:38
by: Nevermore
Putrescine & Co.
what was your most successful reaction? (of course H2S is not valid!! :D )
14-7-2004 at 15:39
by: Nevermore
Putrescine & Co.
the synth over there is too hard, i don't have hydrazine handy neither most of the other chemic ...
14-7-2004 at 13:00
by: Nevermore
Putrescine & Co.
I was thinking about attempting a synth of putrescine, cadaverine, and those nasty smelling stuff..
...
14-7-2004 at 12:05
by: Nevermore
Silver acetylide/nitrate
also you can easily find that is very weak, sometime not able to pierce light cardboard...
this com ...
15-5-2004 at 08:54
by: Nevermore
thermodynamically unstable diamond
diamonds thermodinamically instable?
can you explain better?
diamonds are made of C, they are inst ...
8-3-2004 at 03:56
by: Nevermore
Boy killed in Sweden by homemade explosive
[quote][i]Originally posted by IgnorantlyIntelligent[/i]
Nitroglycerin production is one of the mos ...
26-2-2004 at 13:20
by: Nevermore
Boy killed in Sweden by homemade explosive
those things always happens..
car, gun, explosives..
people just keep thinking they are higlanders ...
23-2-2004 at 12:21
by: Nevermore
What sort of Al and Fe2O3 should I use for Thermite?
[quote][i]Originally posted by theh0ser[/i]
can i get iron oxide by electrolysing water (salt solut ...
22-2-2004 at 11:02
by: Nevermore