Search |
[Next Page] |
Ball mill grinding material (making metal balls - ZA-27) I use hard cast .54 caliber balls. These are soft lead with added tin. I have used the same balls fo ... |
21-9-2017 at 08:37 by: highpower48 |
Candles question Soy Wax is also used in modern candles.
|
17-9-2017 at 08:18 by: highpower48 |
Tour My Lab I have a decent sized lab space approx 10'x10', with two 8 foot work benches that I have built into ... |
17-7-2017 at 10:21 by: highpower48 |
New to chemistry, looking for some ideas On soap making..my wife and I are soapmakers, we have a small business doing so. Main reason I got i ... |
8-7-2017 at 09:40 by: highpower48 |
How do you powderise substances? Coffee grinder
|
18-6-2017 at 07:03 by: highpower48 |
Firearm Primer Question I have a firearm primer question. I know its not a true chemistry question but it seems interesting. ... |
13-5-2017 at 15:01 by: highpower48 |
Iodine purchasing I am in the need of around 100 grams of elemental Iodine. I know I can make it, I have in the past. ... |
2-5-2017 at 09:07 by: highpower48 |
37% hydrochloric acid Where is the least expensive place to buy 37% hydrochloric acid. From what I'm seeing it seems aroun ... |
24-4-2017 at 10:41 by: highpower48 |
Dark Sulfuric Acid By the way the acid came from Duda Diesel |
24-3-2017 at 17:46 by: highpower48 |
Dark Sulfuric Acid Last summer I bought a couple 850ml 98% sulfuric acid that came plastic bottles. I haven't needed th ... |
24-3-2017 at 17:01 by: highpower48 |
What states still sell Toluene? Up until last year could still buy it in quart containers at Lowe's and Home Depot here in NC. Almos ... |
22-3-2017 at 10:42 by: highpower48 |
Doug's Lab This might be the wrong forum for this post, if so please place in the right one.
Anyone know wha ... |
15-3-2017 at 12:25 by: highpower48 |
eBay Discloses Your Bidding History Think only thing I've ordered that might be an issue 100 grams of iodine, was cheaper to buy than ma ... |
15-3-2017 at 11:55 by: highpower48 |
Heat bendable glass tubes For a US retailer in small quantities try Home Science Tools |
1-3-2017 at 10:02 by: highpower48 |
Nitric acid diffuculties Maybe wrong but potassium nitrate is very cheap, lots cheaper than cutting open cold packs. I'm not ... |
27-2-2017 at 09:50 by: highpower48 |
DCM from paint stripper problems I believe it was Nile Red or Nurdrage in one of there videos said they used kerosene for clean-up. |
17-2-2017 at 11:11 by: highpower48 |
DCM from paint stripper problems [rquote=474922&tid=72286&author=dactyl]@JJay
One time I found that when I had little aceton ... |
17-2-2017 at 11:07 by: highpower48 |
Chinese Hotplate/Stirrers Look at this on eBay http://www.ebay.com/itm/232092408590 |
29-12-2016 at 18:34 by: highpower48 |
Chinese Hotplate/Stirrers Will do so when I get home. Phone app does not give me a url.
|
29-12-2016 at 17:27 by: highpower48 |
Chinese Hotplate/Stirrers Has anyone tried the $100.00 Chinese Hotplate/Stirrers? Are they worth the price? |
29-12-2016 at 15:46 by: highpower48 |
electrical advice needed: motor fuse No, not really. You should or replaced it with 10 amp fuse. By replacing it with a higher rated fuse ... |
4-9-2016 at 19:17 by: highpower48 |
New Distillation Set-up Questions Looking at the photos the ground glass joints don't look ground. The normal frosting is not there. T ... |
4-8-2016 at 16:19 by: highpower48 |
Charcoal size for BP - super fine vs "air-float" http://castboolits.gunloads.com/showthread.php?103852-My-homemade-black-powdeR
This will give you ... |
19-7-2016 at 09:02 by: highpower48 |
Weighing paper substitute Freezer paper
|
12-7-2016 at 09:27 by: highpower48 |
HElP PLEASE! Heating Mantle trouble More for my own information. Who made this heating mandle? I only know of one manufacturer in the U. ... |
4-7-2016 at 09:48 by: highpower48 |