Search |
[Next Page] |
Electrolytic DEplating of silver from copper? Thanks! |
12-10-2009 at 07:06 by: jgourlay |
Electrolytic DEplating of silver from copper? Gents: I have a whack of silver plated copper bar. I want to melt this bar down and toss in a teas ... |
12-10-2009 at 05:54 by: jgourlay |
Careers in chemistry Rattata: +1 on JohnWWW's general path of advice. I'll add a couple of thoughts:
1. Chemical En ... |
26-8-2009 at 04:04 by: jgourlay |
Hydrogen Peroxide Storage? Stirring rod sounds fine....except for a one gallon jug, which is a two handed operation for sure. |
19-8-2009 at 12:13 by: jgourlay |
'splain something to me please about water freezing Everado: sometimes you gotta thump it hard. Open the lid, however, and it goes right off every tim ... |
19-8-2009 at 11:30 by: jgourlay |
Hydrogen Peroxide Storage? Barium, do you know of any videos showing the right technique for that pouring? By "right technique ... |
19-8-2009 at 10:48 by: jgourlay |
'splain something to me please about water freezing Gents, here in the office we have a little college refrigerator containing a tiny freezer compartmen ... |
18-8-2009 at 14:02 by: jgourlay |
Hydrogen Peroxide Storage? Ozone: thanks. So I'm thinking I need a dedicated pipette to transfer from the main bottle to the ... |
18-8-2009 at 12:08 by: jgourlay |
Hydrogen Peroxide Storage? Good. Confirms what I thought.
Any problems storing Peroxide, Sulfuric Acid, and Nitric Acid all ... |
18-8-2009 at 07:03 by: jgourlay |
Anyone in East texas need HNO3 and/or H2SO4? Gnit: I'm in houston and could take some of that off your hands! |
18-8-2009 at 07:01 by: jgourlay |
Hydrogen Peroxide Storage? Gents: what is the best method for long term (several year) storage of 35% H202? |
18-8-2009 at 03:50 by: jgourlay |
Vacuum Bell???? I'm stoopid: I have all that at home. Thanks for bringing my attention to the obvious! |
17-8-2009 at 10:10 by: jgourlay |
Vacuum Bell???? Gents:
I need a vacuum bell, but all the ones I find online are REALLY expensive. Anyone here ha ... |
17-8-2009 at 08:22 by: jgourlay |
Detecting lead in brass? Asking this question on behalf of someone over at backyardmetalcasting.com
Is there a (cheap and ... |
5-8-2009 at 09:44 by: jgourlay |
A great demo for the kids! Daddy: three answers
1. (the smart ass answer) "At the musuem!"
2. (the sorrowful answer) S ... |
20-7-2009 at 05:08 by: jgourlay |
A great demo for the kids! Unintentional, thanks. However, it's much better for the kidos if they see a stone being ground up. ... |
7-7-2009 at 05:44 by: jgourlay |
A great demo for the kids! Gents, I do science demo's across a number of different fields for little kids. Note that I keep t ... |
2-7-2009 at 09:05 by: jgourlay |
Why does Fusion work? 12ax7: gravity does work, understood. But what is gravity that it does not run out of the ability ... |
22-6-2009 at 05:10 by: jgourlay |
Interface betwixt condenser and vessel? Ref Matl? Thanks! |
22-6-2009 at 04:59 by: jgourlay |
Interface betwixt condenser and vessel? Ref Matl? [rquote=155531&tid=12398&author=UnintentionalChaos]I think he's saying that he has a non-gro ... |
20-6-2009 at 18:56 by: jgourlay |
Help me deplate something [rquote=155462&tid=12392&author=watson.fawkes][rquote=155459&tid=12392&author=chlori ... |
20-6-2009 at 18:00 by: jgourlay |
Why are subatomic particles charged? Woelen, your reply reinforces and idea I've had for a while. The obvious part is that there is a "p ... |
20-6-2009 at 17:57 by: jgourlay |
Interface betwixt condenser and vessel? Ref Matl? Gents, two questions.
First, I have a condenser with ground glass input/output ports. What is th ... |
20-6-2009 at 05:12 by: jgourlay |
Why does Fusion work? My boss and I were in an alternative energy debate today, and a "fundamental" question came up that ... |
19-6-2009 at 11:46 by: jgourlay |
Help me deplate something Paddywhacker: It's art now....so I'll try it. But thanks for the warning!
Watson: You know, th ... |
19-6-2009 at 05:11 by: jgourlay |
[Next Page] |