preparation of α-nitronaphthalene It looks like you got a clean product.
Generally the first place I go to for solubility data is h ... |
3-3-2026 at 09:33 by: Axt |
preparation of α-nitronaphthalene To be honest the sinking prills surprised me too, and I still don't have an answer for it, other tha ... |
26-2-2026 at 00:47 by: Axt |
preparation of α-nitronaphthalene Attaching the original "just HNO3" reference. They used d. 1.33 (~53%) nitric acid which they descri ... |
25-2-2026 at 10:28 by: Axt |
preparation of α-nitronaphthalene Um, as much as I can appreciate the effort and enthusiasm in this thread it does all seems quite mel ... |
25-2-2026 at 09:37 by: Axt |
Problems detonation of the mixture PETN/NG I've some experience with PETN/NG (penthrinite) and can confirm that contrary to the original litera ... |
11-2-2026 at 08:18 by: Axt |
New Energetic Materials - Current Research I tried again, 5 g DAF was stirred in room temp. 68% HNO3 for 2-3 hrs until it dissolved, then eithe ... |
5-2-2026 at 03:14 by: Axt |
New Energetic Materials - Current Research Are you saying you did receive a precipitate from pouring the water/nitration mixture directly into ... |
3-2-2026 at 14:34 by: Axt |
Exotic Primaries - Complex Salts Here is two translated quotes from Chinese Journal of Universities, (2001), vol. 22, pg. 895. regard ... |
13-1-2026 at 08:11 by: Axt |
Energetic Perovskites Yes, it had turned yellowish-beige however the filtrate turned everything black so I cannot say if i ... |
13-1-2026 at 03:40 by: Axt |
Energetic Perovskites 1 yr old DPPE-1 left exposed on filter paper still fires fine.
I made some ETT (Ethylenediamine D ... |
10-1-2026 at 09:56 by: Axt |
Simple melt-cast carrier 2,4-dinitrophenoxyethyl nitrate (DNPOEN)? [rquote=705220&tid=161448&author=KFeNAT]For some reason, it seems like the images aren't bei ... |
10-1-2026 at 09:26 by: Axt |
Simple melt-cast carrier 2,4-dinitrophenoxyethyl nitrate (DNPOEN)? US1560426A is the patented trinitro analogue https://patents.google.com/patent/US1560426A/en?oq=us1 ... |
20-12-2025 at 09:33 by: Axt |
New Energetic Materials - Current Research Yeh I did stir some DAF in oxone and received a high yield of DAAF, it will respond with a weak snap ... |
13-12-2025 at 13:30 by: Axt |
New Energetic Materials - Current Research Yeh I got to reading the old furazan pre-pub thread https://www.sciencemadness.org/talk/viewthread.p ... |
12-12-2025 at 08:17 by: Axt |
New Energetic Materials - Current Research Difurazanotetrazocine (DFT), 40 mg in a single layer of foil was negative to DDT, just flashed with ... |
11-12-2025 at 10:27 by: Axt |
New Energetic Materials - Current Research Have you entertained the thought of the microwave preparation:
One pot synthesis of DAF from glyo ... |
11-12-2025 at 01:31 by: Axt |
New Energetic Materials - Current Research I had some DAF from ages ago, so I treated 1 gram with TCCA in acetonitrile (1:2 molar eq. in 50 mL ... |
10-12-2025 at 10:22 by: Axt |
Short question / quick answer - Thread Shock isn't independant of heating, it's either referring to pressure (ie. shock) induced heating or ... |
6-12-2025 at 10:42 by: Axt |
Magnetic stirrer with heating, own temperature sensor W2022 AC110/220V Precise Temperature Control 1500W Smart Digital LED Display Thermostat Microcompute ... |
6-12-2025 at 09:05 by: Axt |
DiNitroNeoPentane? He is after something that will colloid with nitrocellulose but act as a stable burn retardant, not ... |
6-12-2025 at 05:29 by: Axt |
Short question / quick answer - Thread The quick answer is adiabatic heating is the primary initiator, but it's a complex question. You cou ... |
1-12-2025 at 23:23 by: Axt |
DiNitroNeoPentane? I'm struggling to see why someone would take interest in making a burn rate modifier or "flame retar ... |
29-11-2025 at 05:13 by: Axt |
Easy SMX Just an update on the melting point, I placed a small portion of naphthalene next to the SMX and slo ... |
25-11-2025 at 23:07 by: Axt |
3,3’-Diamino-5,5’-bis(1H-1,2,4-triazole) and Derivatives Yes, the word "primary" although it implies its action on a secondary seems to have been coopted to ... |
24-11-2025 at 04:50 by: Axt |
3,3’-Diamino-5,5’-bis(1H-1,2,4-triazole) and Derivatives Malonic acid was available locally for some reason, so I gave it a try following procedure in 3rd po ... |
23-11-2025 at 20:01 by: Axt |