H2S04 dissolve silver? Thanks "not_importand" and "Xenoid" for answering.
I am only using between 1 - 1.5% dilute H2S04, ... |
27-12-2007 at 19:50 by: angela_li |
H2S04 dissolve silver? Hi
I was told H2S04 will not dissolve silver, but in my test. I did an XRF test on the ore and f ... |
24-12-2007 at 17:23 by: angela_li |
Dark Green water Help.
Can 1 - 1.5% sulf acid disolve copper and silver in oxide and sulphide ore, if the ore is m ... |
6-12-2007 at 22:15 by: angela_li |
Dark Green water I wish to thank not_important for the help. I think I found the answer. I was using 304 stainless ... |
4-12-2007 at 20:02 by: angela_li |
Chemical Name Hi froot.
Thanks for the help. I found most of the names, then used google translation to find t ... |
3-12-2007 at 05:44 by: angela_li |
Dark Green water Sorry Dale. I think you answered the wrong person.
But thanks for the post.
Angela. |
3-12-2007 at 05:37 by: angela_li |
Chemical Name Hi All !
Can anyone give me a site were I can find the names of these chemical name both English ... |
3-12-2007 at 04:14 by: angela_li |
Dark Green water Hi All.
My expeiment: I am milling the oxide and sulphide ore down to micron's and not heap leach ... |
3-12-2007 at 03:42 by: angela_li |