Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Search
Drying hydrated copper formate
the decomposition in the desiccator was different from the one upon heating it.
When heated, yes it ...
17-3-2016 at 10:32
by: huegene
Drying hydrated copper formate
Small update and Problems:
so for now i have been able to decompose the copper formate to copper, b ...
1-3-2016 at 06:39
by: huegene
H2O2 By Electrolysis
as far as i remember you distill the h2o2 (at low pressure ?) off.
15-1-2016 at 10:13
by: huegene
Sodium Ethyl Sulfate
How did the vaccum filtration go?
By the way i was wondering, is sodium bisulfate soluble in anhyd ...
18-12-2015 at 16:34
by: huegene
Drying hydrated copper formate
I know,
i mean to wirelessly transport energy into the desiccator having a reception coil inside or ...
7-12-2015 at 11:02
by: huegene
Drying hydrated copper formate
It took me some more searching but I've finally got some numbers. This patent: http://www.freepatent ...
3-12-2015 at 16:31
by: huegene
Drying hydrated copper formate
Hi everyone,
I intend to deposit copper into printed circuit board holes (aka through hole plating ...
3-12-2015 at 11:46
by: huegene
How can i make a surface conductive without going mad or broke?
I am struggeling with the same problem.
Recently i stumbled upon a few promising methods.
Escala ...
1-12-2015 at 14:54
by: huegene