Sciencemadness Discussion Board

fuckin plastic piece of shit hoses

daeron - 13-6-2006 at 03:00

i almost lost my life right now. was working with a reactor with a heating jacket 210C, heated by mineral oil from the termostat, pumped by 0.5 -1m/s.
and the little fuckin retarded techincian idiot supplied me with a hose that can stand up to 75C.
i dont need to explain what happened next, the hose melted, the oil started bursting all over the lab, i got burns over my chest, the reactor cracked, the mixture caught fire, my lab coat started to burn, my gloves melted....FUUUUUCK.
im standing in the middle of some 5 m2 of oil around me..

luckily i was fast enough to put out the fire and strip. i hope the burns are not too dangerous, there are only a few blisters, and some part of the melted glove in my fuckin hand. and not to mention the embarresment when the firemen ran in and found me in my boxershorts and undershirt trying to put out the fire...

goddamnit, I HATE FUCKIN TECHINICIANS.

sorry for the bitching but i had to let off some steam, since officaly im responcible for this shit....im off to the doc

peace, oil, sand and soap.

[Edited on 13-6-2006 by daeron]

Saerynide - 13-6-2006 at 03:44

Wow. That sucks. Glad you're ok.

Btw, fire the bastard.

chochu3 - 13-6-2006 at 04:52

That's why an authority always over checks the work of a techinician.

Technician

MadHatter - 13-6-2006 at 10:16

Agreed. Fire the incompetent fuck. Also, with the next technician you get, carefully
review the setup. Glad your OK.

unionised - 13-6-2006 at 12:43

Fire the guy who didn't train the tech.

Nerro - 13-6-2006 at 13:38

If you do such work it can't hurt to check the items supplied to you, you may want to do that from now on.

Jope you'll be ok though, burns really suck. I once melted a bit of plastic into the skin of my hand, took ages to come off.

unionised - 14-6-2006 at 11:30

I hope you are OK and have calmed down enough to see the funny side of
"I HATE FUCKIN TECHINICIANS"
well fuck someone else then.

BTW, if the oil was at 75C when the hose failed, what cracked the reactor and what started the fire.

Nerro - 14-6-2006 at 13:12

Quote:
Originally posted by unionised
I hope you are OK and have calmed down enough to see the funny side of
"I HATE FUCKIN TECHINICIANS"
well fuck someone else then.


BTW, if the oil was at 75C when the hose failed, what cracked the reactor and what started the fire.
LOL!

daeron - 22-6-2006 at 03:39

thx to all who replied, the person altho she was HOT was fired, so no fucking of technicians there. got burns over my chest and some plastic in my right arm but otherwise im okay. this was a good lesson.

Technician

MadHatter - 22-6-2006 at 08:01

Ashame she's real HOT ! I'd say she owes you a fuck for the misery she put you through
as a contrite apology to the agrieved. :D:D:D

DeAdFX - 22-6-2006 at 10:29

If your going to fuck people at your work place at least make sure that they can give you a promotion otherwise its not worth the time to take out the knee pads...;)

[Edited on 22-6-2006 by DeAdFX]

andersderis - 3-7-2006 at 13:00

fire tha bitch!!!

Adar - 8-7-2006 at 05:50

Could you show a picture of the cracked reactor and point out the hose? It could be useful to avoid future mishaps for other people (and be quite intresting).