I reacted aluminium foil with muriatic acid until no more aluminium would react. The reaction formed a gray foam of bubbles. I left the beaker out overnight with a watch glass over it to allow any remaining aluminium flakes to react. In the morning i found there was still a gray precipitant. It measured a very low pH (cabbage indicator solution and pH paper). The precipitant did not dissolve with water or HCl. The precipitant seemed to float on the solution but i am not sure of that. Filtration yielded a gray filtrate.

To the best of my knowledge aluminium chloride is yellow and soluble in water. I don't think it was aluminium because that would have reacted upon the addition of more acid. Perhaps an impurity in the metal. Any insight on what the precipitant may be and if this is normal would be appreciated. Furthermore , why does the reaction of aluminium and HCl turn gray?

Chemkid




View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 21-10-2007 at 10:53


Could be silicon and other impurities.

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
Polverone
Now celebrating 21 years of madness
*********




Posts: 3186
Registered: 19-5-2002
Location: The Sunny Pacific Northwest
Member Is Offline

Mood: Waiting for spring

[*] posted on 21-10-2007 at 11:20


If you still think this is a mystery, consider continuing discussion in the mystery reaction thread.



PGP Key and corresponding e-mail address
View user's profile Visit user's homepage View All Posts By User

  Go To Top