Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Ca(ClO)2 synthesis
Ballermatz
Harmless
*




Posts: 19
Registered: 17-7-2007
Member Is Offline

Mood: No Mood

[*] posted on 2-12-2007 at 15:35
Ca(ClO)2 synthesis


I havent found any synthesis on the forums - probably because Ca(ClO)2 is easily available off the shelf. Well not to me, so I need to make some. Starting materials I have at hand are TCCS+HCl for chlorine generation and 500g of Ca(OH)2.

In a chemistry book it says that I have to pass chlorine into the Ca(OH)2 solution, then cool it down until the hypochlorite crystallizes, but it doesnt give any details. Which temperature must the Ca(OH)2 solution have? How do I dry the Ca(OH)2 (which probably comes out in a hydrated form) without decomposing it?
View user's profile View All Posts By User
chloric1
International Hazard
*****




Posts: 1238
Registered: 8-10-2003
Location: GroupVII of the periodic table
Member Is Offline

Mood: Stoichiometrically Balanced

[*] posted on 2-12-2007 at 18:25


Ca(OH)2 is only slightly soluble in water so it must be constantly agitated while chorinated. Chlorinate until it is saturated with chlorine. When you are done chill in the freezer but do not freeeze. Your hypochlorite should deposit.



Fellow molecular manipulator
View user's profile View All Posts By User
chemkid
Hazard to Others
***




Posts: 269
Registered: 5-4-2007
Location: Suburban Hell
Member Is Offline

Mood: polarized

[*] posted on 2-12-2007 at 19:10


Anyone have any idea on the normal purity of store bought hypochlorite in the form of bleach? How about other methods of synthesis? Never boguht any bleach becuase i'm concerned about fillers/binders/dyes/crap.

Chemkid




View user's profile View All Posts By User
BromicAcid
International Hazard
*****




Posts: 3315
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline

Mood: Rock n' Roll

[*] posted on 2-12-2007 at 19:11


I recall something about reacting chlorine with trays of lime as one of the older preparations. Pretty sure I can find some more details if that isn't sufficient to jog someone's memory around here.



Shamelessly plugging my attempts at writing fiction: http://www.robvincent.org
View user's profile Visit user's homepage View All Posts By User
not_important
International Hazard
*****




Posts: 3873
Registered: 21-7-2006
Member Is Offline

Mood: No Mood

[*] posted on 2-12-2007 at 19:39


Quote:
Originally posted by chemkid
Anyone have any idea on the normal purity of store bought hypochlorite in the form of bleach? How about other methods of synthesis? Never boguht any bleach becuase i'm concerned about fillers/binders/dyes/crap.


Depends. Plain bleach is generally a solution of NaOCl, NaCl, and NaOH. Water is the filler, cheapest one around. Scented ones generally announce themselves on the label, avoid them and the thickened types sometimes showing up as "no spill"

Yes, bleaching powder was made using trays of the hydroxide or oxide, the hydroxide perhaps being dampened, otherwise with some steam included with the chlorine. There's a lot of 19th century books on practical or industrial chemistry that describe this. This is a little more recent on
http://books.google.com/books?id=MQA5AAAAIAAJ&pg=PA202&a...
View user's profile View All Posts By User