Lampblack in place of charcoal?
Does anyone know if lampblack can be substituted for charcoal in black powder and similar low explosives?
Hodges
|
|
|
JDP
Harmless
Posts: 43
Registered: 31-10-2003
Location: CA
Member Is Offline
Mood: |:booM
|
|
Yes, charcole is actually a better fuel for Black powder and the like, although I've never worked with lampblack befor. I would amagin charcole
is alot cheaper too.
[Edited on 6-1-2004 by JDP]
~JDP
|
|
|
KABOOOM(pyrojustforfun)
Hazard to Others
 
Posts: 254
Registered: 12-10-2002
Location: Iran (pseudoislamic dictatorship of)
Member Is Offline
Mood: exuviating!
|
|
I have tried
it SUCKS in most composition. I don't know why it is so inert to ignition. sulfurless black powder didn't burn at all! I heated some on bare
flame the nitrate melted and started to bubble! but no ignition! . normal meal
powder with charcol substituted with lampblack burns very slowly and veeeery smoky
|
|
|
Iv4
Hazard to Others
 
Posts: 312
Registered: 28-5-2003
Member Is Offline
Mood: No Mood
|
|
Depends
Could you please give more details?
Like stated above its usefull for making smoke(cant remember of hand but sugar/lampblack/some chlorate/some rubber makes a nice smoke mix).
My atempts at a BP were failed as well but I have a theory,lampback being so fine pure has more energy.So more oxidizer maybe needed.Though considring
the bubling could be the opsite.
|
|
|
Mr.O-Nitrate
Harmless
Posts: 25
Registered: 16-10-2003
Member Is Offline
Mood: No Mood
|
|
.
It's carcinogenic..
|
|
|
hodges
National Hazard
  
Posts: 525
Registered: 17-12-2003
Location: Midwest
Member Is Offline
|
|
| Quote: | Originally posted by Iv4
Could you please give more details?
Like stated above its usefull for making smoke(cant remember of hand but sugar/lampblack/some chlorate/some rubber makes a nice smoke mix).
|
If one substitutes lampblack where charcoal is called for, it is not going to work, right? I mean like for example to reduce CuO to Cu, to make
various firework and rocket powders, etc.
I have a friend with some black powder that he says is lampblack and was wondering what use it might be.
Okay, guess I need to check out Adiabatic's files and see what they have to say about this. I searched through usenet and the only uses I saw
for lampblack there was making sparks in certain types of fireworks.
Hodges
|
|
|
overseer
Harmless
Posts: 24
Registered: 31-12-2003
Member Is Offline
Mood: Relaxed
|
|
Quite a while ago, I tried to use soot instead of charcoal. I had a bag full of soot after cleaning a metal chimney tube of a wood-burning furnace,
and I wanted to see whether it would work. This would provide a free source of relatively pure and finely divided carbon, suitable for the purpose (or
so I thought). Unfortunately, I must report a lack of success.
The major problem when working with soot was that I couldn't get it wet before blending. This is easily seen if You deposit some soot on a test
tube, e.g. by using a candle flame, and when it cools down, immerse it in a glass of water: some soot falls off and floats on the surface, some
remains on the tube, but none gets wet. It was difficult enough to admix finely pulverized sulfur, but soot..... A "fair success" was
ultimately achieved by admixing some flour-based gel, obtained by boiling some flour in water, and later vigorously shaking this in a bottle with lots
of soot. When this mixture was blended, it was poured out and left to dry, and later re-pulverized in a mortar, in a similar fashion as with the
charcoal. However, this fuel could never be completely dried, and consequently, could not burn very fast. I didn't find any other suitable
wetting agent, though I tried many. Working with this was painstaking though, as the soot is very light and easily flies, is difficult to measure,
gets things messy etc.
The "flour-bound fuel" could be used in a furnace as a very good fuel, but that's all it was good for. Later I learned lampblack is
used in fireworks for making bright, finely dispersed "stars" that burn bright but slow.
I speculated on why the results were so poor, but I couldn't be sure my speculation was correct. I didn't encounter this topic in the
literature, so if someone else did, I'd appreciate the input. I tried to identify the main differences between the soot I used and standard
charcoal. The two most obvious were the chemical composition and mixing properties. The fact that the soot could not be wetted by itself, led to the
conclusion that it couldn't be intimately blended with other ingredients (chiefly the oxidizer) so the contact surface would be small. Second,
the charring procedure retains catalytically active metal oxides in charcoal, whereas the soot is almost pure carbon (and perhaps some incomplete
burning products): when lightly compressed and exposed to Bunsen heating in a ceramic dish, it ignites (shines) and almost completely burns leaving
very little residue.
My conclusion at the time was that the lack of catalytic action of metal oxides that promote burning could be the cause of soot being such a slow
burning fuel when compared to charcoal. I remember the old experiment of igniting sugar: it burns very well in contact with wood or cigarette ash, but
only melts and carbonizes if ignited alone. Now that someone mentioned that, it appears logical that the high carbon content in soot would require
more oxidizer, as well. As to the contact surfaces, charcoal is a good adsorbent owing to large contact surfaces its porous structure has, so these
two might contribute to the observed results. I speculate the repelling of water might indicate the soot repelling the hot gases during combustion as
well, which could hinder the process. Sulfur melts at elevated temp, so the analogy would not apply. Again, this is just my speculation and may not be
true. If someone reported success with this fuel, please provide some input about the procedure they used. It would certainly be great to have access
to a scanning electron microscope as the one described in the technical report above, to see what really happens in there, but...
|
|
|
overseer
Harmless
Posts: 24
Registered: 31-12-2003
Member Is Offline
Mood: Relaxed
|
|
| Quote: | Originally posted by Adiabatic
Lamblack from a chimney will be anything but pure. Perhaps you could have wetted it with EtOH or similar.
I'll try accumulate sufficient carbon from burning acetylene to test it myself.
|
Yes, I'm aware of that, but as I said, the goal was to obtain cheap fuel. I also tested it to see how much residue it would leave after burning
all the carbon out, as I explained. It left almost none . . .
I didn't want to use pure lampblack because it was always too expensive compared to charcoal, and I thought my experience with chimney soot would
apply to lampblack as well, at least in part . . . 
And yes, I forgot, I've seen mentioning isopropyl-alcohol somewhere in the literature, which would be similar to EtOH You proposed for the
purpose, but again, "reasons of economy..." 