Gents, a warning on the inexpensive faceted alchohol lamps that are currently for sale on some sites. Long story short, they are made from non-lab
grade glass.
The upshot is that after about 5 minutes of use, they become hot enough to cause the glass to crack through. The crack then starts to leak fluid that
immediately catches on fire.
This is really great, especially when (skeptical) mom is watching you teach science to the kids ![:mad:](./images/smilies/mad.gif)
Fortunately, it didn't SHATTER until I got it out to the yard to a sandy spot.
|
|
panziandi
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 490
Registered: 3-10-2006
Location: UK
Member Is Offline
Mood: Bored
|
|
Blimey that could easily have been very much worse! Good warning!
|
|
undead_alchemist
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 189
Registered: 12-1-2007
Location: Vancouver, Canada
Member Is Offline
Mood: Tired, Cleaning up corporate messes at work!
|
|
The better made alcohol laps from one supplier cost $7.00 each list.
|
|
jgourlay
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 249
Registered: 9-7-2008
Member Is Offline
Mood: No Mood
|
|
Undead: what's your source? Also, are those micro butane torches "better".
I'm looking, of course, for the safest source of gentle heat. But I like the alcohol lamp because well, it uses a cheap fuel.
|
|
chemkid
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 269
Registered: 5-4-2007
Location: Suburban Hell
Member Is Offline
Mood: polarized
|
|
I have used an alcohol burner for up to twenty consecutive minutes and had no problem. In fact, i could pick it up comfortably with my hands. The wick
on mine has a metal sleeve which elevates the burning to about 2cm above the actual glass.
[Edited on 27-9-2008 by chemkid]
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
I've never heard of such a thing. I used an alcohol lamp for years as a kid that came with my Gilbert chemistry set with never a problem. It seems
strange that the glass would even get that hot. It seems like most all the heat would be from the flame cone up. But I haven't used one in a long
time.
|
|
ScienceSquirrel
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
I have used alcohol burners in the past with no problems.
Go for a good quality burner for medical use or similar and you should be OK.
Butane torches are OK but they need a high fuel air ratio to ignite.
After that you have to throttle them down to get a cooler flame otherwise they will crack glass.
|
|
HydroCarbon
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 77
Registered: 7-7-2008
Location: Anytown, USA
Member Is Offline
Mood: No Mood
|
|
I had the same thing happen to me when I was using a cheap alcohol lamp as well. I had it lit for only about 15 minutes, first time using, and I
heard a snap. I didn't know it had cracked until I put it out after hearing the snap and saw the top move. Luckily I had only filled it half way and
the crack was at the very top near the metal cap.
People should definitely watch out for this, as it could be extremely dangerous if a full lamp cracked to spill ignited alcohol all over the place; or
vapor escaping from the crack was ignited.
I got a micro butane burner to replace the alcohol lamp and it works great.
I would like to try one of those wickless alcohol lamps, though, as alcohol is much cheaper to burn than butane.
[Edited on 29-9-2008 by HydroCarbon]
|
|