Rattata2
Harmless
Posts: 35
Registered: 22-6-2009
Member Is Offline
Mood: No Mood
|
|
How to separate copper and carbon powder?
I have a mixture of copper and carbon powder, the copper being made by reducing copper (II) oxide by reducing under heat with the carbon. I would like
to separate the copper from the carbon powder (and perhaps any oxide left over, but that's later.) Is there any feasible way to do this?
|
|
inspector5
Harmless
Posts: 14
Registered: 9-9-2010
Member Is Offline
Mood: No Mood
|
|
I may be wrong and if I am someone smarter will surely correct me but the first thing I would try would be to suspend the mixture in water and wait a
little and decant off what will hopefully be the carbon suspended then repeat until you remove most (or enough) of the carbon. How long to wait will
have to be determined by observation. I believe that should work fairly well at separating the carbon out given a roughly 4:1 ratio of
densities between copper:carbon but you will probably have any remaining copper(II) oxide spread between the 2 though I would predict
predominately in with the metallic copper.
|
|
peach
Bon Vivant
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1428
Registered: 14-11-2008
Member Is Offline
Mood: No Mood
|
|
It's not magnetic, they're both solids, they're finely mixed... that makes it tricky to physically separate them.
I was going to suggest you salt the copper into solution and filter it away, but that's going to give you salt back which will need reducing again.
If you can handle gases, you may be able to reduce the copper with monoxide, by heating the carbon, blowing air gently through it and out into a tube
with the warmed copper in it.
Haven't checked.
Be VERY careful with monoxide.
It is odourless, metabolically and neurologically toxic.
There are numerous gases that will function as a reducing atmosphere.
Hydrogen can be used for this. You could generate a decent amount by reacting tin foil (what is backward brits call kitchen foil, and which is
actually aluminium) with sodium or potassium hydroxide.
[Edited on 5-1-2011 by peach]
|
|
Saerynide
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline
Mood: Ionic
|
|
Like Inspector said, perhaps putting the powder into a long glass cylinder like 1 L graduated cylinder with water and shaking the whole thing. When
it setttles, the copper should be on the bottom with the carbon on the top layer. CuO will be somewhere in between, but should be less dense than
copper metal. Then you can syphon off the carbon layer like how you clean a fish tank. Maybe change the density of the medium if water isnt
providing such a good separation.
"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to...
satisfy any applicable law, regulation or legal process"
|
|
The WiZard is In
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1617
Registered: 3-4-2010
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Saerynide ![](images/xpblue/lastpost.gif) | Like Inspector said, perhaps putting the powder into a long glass cylinder like 1 L graduated cylinder with water and shaking the whole thing. When
it setttles, the copper should be on the bottom with the carbon on the top layer. CuO will be somewhere in between, but should be less dense than
copper metal. Then you can syphon off the carbon layer like how you clean a fish tank. Maybe change the density of the medium if water isnt
providing such a good separation. |
Put in a long cylinder put a piece of pipe/tubing down to the bottom
and run air/or water through it. Adjust the speed so that the
lightest/least dense solid floats up/out. This process can - has been
nuanced for hundreds of years, principle to separate metallic ores.
|
|
cyanureeves
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
that chemistry fellow with the white beard on youtube told a viewer that copper salts can be smelted with addition of carbon.mine just go up in
smoke.unless he only meant the carbonate.
|
|
Jor
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 950
Registered: 21-11-2007
Member Is Offline
Mood: No Mood
|
|
Burn it and reduce the copper oxides.
|
|
hissingnoise
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3940
Registered: 26-12-2002
Member Is Offline
Mood: Pulverulescent!
|
|
Whoops! Ever decreasing circles . . .?
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
You could heat it and oxidise the carbon with CO2 or water but that would give you CO which isn't nice stuff to work with. If you burned the mixture
to CuO and CO2 then reduced the CuO with alcohol vapour you would get nice clean copper.
Jor's suggestion isn't as silly as it might have sounded
|
|