Thermite casting
So I was wondering, has anyone tried or know anything about casting iron with thermite?
I've ran the thermite reaction before with no problem - the molten iron falling on to dry sand and giving a pretty lump of shiny bluish steel... but
what would be a suitable mold material without worrying about a steam explosion? Sand/fireclay and oil?
I'm mostly interested in casting small objects, about the size of large coins, so I think it should be relatively easy if a suitable mold material is
found.
I've alloyed and casted silver ingots once using someone else's propane torch, but I don't have one to borrow anymore and it wouldnt be able do iron
anyway...
This would be a rather expensive way to cast... but I'd like to try out of curiousity and symbolism of merely having cast said objects this way.
[Edited on 7/1/2011 by Saerynide]
[Edited on 7/1/2011 by Saerynide]
"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to...
satisfy any applicable law, regulation or legal process"
|
|
|
The WiZard is In
International Hazard
   
Posts: 1617
Registered: 3-4-2010
Member Is Offline
Mood: No Mood
|
|
A/ Google sand casting.
B/ Gas Torch and Thermit Welding
Ethan Viall
McGraw-Hill 1921
I own an original copy you can DL/read yours at
Google.com/books
http://tinyurl.com/3q8bcyk
Page 379 & ff.
|
|
|
Mr. Wizard
International Hazard
   
Posts: 1042
Registered: 30-3-2003
Member Is Offline
Mood: No Mood
|
|
I have used commercially available thermite products, which I will not name, to weld ground wires to grounding rods. The container for the reaction
and the mold to form the welded portion were made of a graphite block. They also made a 'one use' device that was not reusable. The thermite did
contain a lot of copper, and was rather quick. A key to a successful weld was to use a thin barrier of a metal disk between the reaction chamber and
the mold section. The purpose of the metal barrier was to allow time for the more dense metal to accumulate under the molten oxide layer. The molten
pure metal would finally burn through the separator and flow into the chamber where the wire and the ground rod were contained. The heat from the
molten metal would bond the rod to a heavy wire with a corrosion proof connection. If the mold was worn, the material damp or moist, or if the wrong
kind of metal disk was used, the whole process was ruined. The disk was crucial, and without it alumina and metal would flow into the mold and form a
real mess.
If you are casting small items you might think about making a mold from graphite, but I think sand with a binder is more often used commercially.
It may be strictly correct to say 'iron casting', as it is iron, but in common terms what you would be getting is more of a steel. Cast iron in common
English is an alloy containing large quantities of carbon and silicon. Of course your thermite product could have a custom alloy of your own choice.
|
|
|
Saerynide
National Hazard
  
Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline
Mood: Ionic
|
|
Thanks for the great information! I was wondering about that last night... how to keep the slag from going into the mold first? At first, I was
thinking maybe some kind of grate to skim off the floating slag as everything flowed along, but it might lose too much heat in the process... and
there isnt quite the luxury of a controlled pour from a crucible 
I remember when very small amts of thermite was used, all that comes out is slag or some mixed useless mess, but when I ran about 130 grams, I didn't
have a problem with the slag mixing with the metal. I cant remember which came out first, but when everything cooled, I had a little geode of porous
blackish grey material, and when broken with my hands, revealed a round lump of shiny steel inside (I still have it). I used the 2 flower pot method.
Of course, this method as is wouldnt be quite good enough for casting...
I imagine the reaction chamber must have some sort of cone shaped bottom where the disk would be placed so the molten material would have time to
collect and phase-separate? Any idea what the disk might be made of? Copper? Nickel? Steel?
I previously thought about graphite, but I think I'll have to stick to sand, since I want to cast (almost exact) copies of objects I already have...
BTW, was this commercial kit expensive? I wouldnt mind buying and using it if it's already preoptimized for the job. Most of the commerical products
I see are on a rather large scale for rail repair, but I guess I can still look to them for engineering inspiration - scaling down is much easier than
scaling up 
[Edited on 7/2/2011 by Saerynide]
"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to...
satisfy any applicable law, regulation or legal process"
|
|
|
watson.fawkes
International Hazard
   
Posts: 2793
Registered: 16-8-2008
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Saerynide  | | BTW, was this commercial kit expensive? I wouldnt mind buying and using it if it's already preoptimized for the job. | The Wikipedia page exothermic welding lists the major brand names.
|
|
|
The WiZard is In
International Hazard
   
Posts: 1617
Registered: 3-4-2010
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Saerynide  |
I imagine the reaction chamber must have some sort of cone shaped bottom where the disk would be placed so the molten material would have time to
collect and phase-separate? Any idea what the disk might be made of? Copper? Nickel? Steel? |
Steel. Try a small ceramic flower pot, just be set up so that if
it breaks you don't set your house a light.
Use the flower pot as a mold and make a Papier-mâché
thermit holder good for one use.
|
|
|
argyrium
Hazard to Others
 
Posts: 123
Registered: 3-2-2008
Location: Pacific
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by The WiZard is In  | Quote: Originally posted by Saerynide  |
I imagine the reaction chamber must have some sort of cone shaped bottom where the disk would be placed so the molten material would have time to
collect and phase-separate? Any idea what the disk might be made of? Copper? Nickel? Steel? |
Steel. Try a small ceramic flower pot, just be set up so that if
it breaks you don't set your house a light.
Use the flower pot as a mold and make a Papier-mâché
thermit holder good for one use. |
It may also be a really good idea to dry the flower pot out well in an oven before doing this. Less likely to crack from steam. Unused/new pots (no
salts) are also a good idea. Clays can hang onto H2O quite tenaciously.
|
|
|