Phantom
Harmless
Posts: 43
Registered: 26-4-2011
Member Is Offline
Mood: AUDENDUM EST,FORTES AUDIUVAT IPSE DEUS
|
|
DPPP ReSearch, synthesis etc.
So everybody know DPPP and it is a really interesting stuff. It's nearly impossible to make it but with some experience and research
I will try it.
Let's refresh our knowledge about DiPhoronePentaPeroxide for those who never heard about it or just forgot it.
This explosive really famous mostly because it's VoD which is around 9000m/s
Made from the same chemicals like TATP> Acetone, H2O2 and HCl
Theory.. HCl changes Acetone into Phorone (yellow green) and then into Pentachlorophorone which is an oily dark reddish liquid. When H2O2 is added the
Cl2 is split away and is replaced by the (O2)5...
The question is: Somebody ever had made or had experience with this stuff?
Any synthesis tips?
I know YouTube is not the right place for synthesis and stuff but I found a video about DPPP. It looks like a load of crap.
http://www.youtube.com/watch?feature=endscreen&NR=1&...
But here is pt. 2 which is a little bit more interesting.
http://www.youtube.com/watch?v=tCN6E2YWLYg&feature=chann...
Maybe that is really DPPP? Hope he will show us some flame and shock tests.
So let's figure out a good synthesis for this project.
[Edited on 13-12-2011 by Phantom]
|
|
Rosco Bodine
Banned
Posts: 6370
Registered: 29-9-2004
Member Is Offline
Mood: analytical
|
|
http://www.youtube.com/watch?v=dP5iVZHm1TE Secret Journey
|
|
Phantom
Harmless
Posts: 43
Registered: 26-4-2011
Member Is Offline
Mood: AUDENDUM EST,FORTES AUDIUVAT IPSE DEUS
|
|
Whats the point of that?
|
|
Rosco Bodine
Banned
Posts: 6370
Registered: 29-9-2004
Member Is Offline
Mood: analytical
|
|
Exactly
http://www.youtube.com/watch?v=0mgSCKXSp9M King Of Pain
[Edited on 13-12-2011 by Rosco Bodine]
|
|
KemiRockarFett
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 84
Registered: 23-7-2004
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Phantom ![](images/xpblue/lastpost.gif) | So everybody know DPPP and it is a really interesting stuff. It's nearly impossible to make it but with some experience and research
I will try it.
Let's refresh our knowledge about DiPhoronePentaPeroxide for those who never heard about it or just forgot it.
This explosive really famous mostly because it's VoD which is around 9000m/s
Made from the same chemicals like TATP> Acetone, H2O2 and HCl
Theory.. HCl changes Acetone into Phorone (yellow green) and then into Pentachlorophorone which is an oily dark reddish liquid. When H2O2 is added the
Cl2 is split away and is replaced by the (O2)5...
The question is: Somebody ever had made or had experience with this stuff?
Any synthesis tips?
I know YouTube is not the right place for synthesis and stuff but I found a video about DPPP. It looks like a load of crap.
http://www.youtube.com/watch?feature=endscreen&NR=1&...
But here is pt. 2 which is a little bit more interesting.
http://www.youtube.com/watch?v=tCN6E2YWLYg&feature=chann...
Maybe that is really DPPP? Hope he will show us some flame and shock tests.
So let's figure out a good synthesis for this project.
[Edited on 13-12-2011 by Phantom] |
The two links was 100 % shit.
1) If DPPP exists it will probably be as sensitive as all peroxides due to the -O-O weak bond.
2) To low density and energy content for the stated 9000 m/s.
Pure H2O2 is in 6000-6500 m/s at 1.450 g/cm3 (20 °C, pure)
The DPPP have been up before and I think everybody tried it out get some TATP.
|
|
Bot0nist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1559
Registered: 15-2-2011
Location: Right behind you.
Member Is Offline
Mood: Streching my cotyledons.
|
|
http://www.sciencemadness.org/talk/viewthread.php?tid=179
Use the forum search engine!
Don't get your hopes up. TCAP is what you'll get every time IIRC.
U.T.F.S.E. and learn the joys of autodidacticism!
Don't judge each day only by the harvest you reap, but also by the seeds you sow.
|
|
Adas
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 711
Registered: 21-9-2011
Location: Slovakia
Member Is Offline
Mood: Sensitive to shock and friction
|
|
I see no way it can be formed. Even the pentachloride is impossible to form. Maybe dichloride, made by addition of HCl onto the double bonds, but can
H2O2 push that chlorine away (as HCl)? I tried this, but I got a deep red resin, no peroxide formed at low temperatures (dry ice bath). In earlier
experiments, yellow (phorone-contaminated) TATP formed. I think we should try to make more realistic explosives.
This is my video I made a few months ago.
http://www.youtube.com/watch?v=EOlXlJeWUmA
[Edited on 14-12-2011 by Adas]
|
|