Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Urea Recrystallization
Hexavalent
International Hazard
*****




Posts: 1564
Registered: 29-12-2011
Location: Wales, UK
Member Is Offline

Mood: Pericyclic

[*] posted on 9-2-2012 at 11:41
Urea Recrystallization


I recently heated up 700g of urea in 100ml of water to recrystallize it . . .but, soon after I smelt a strong odour of ammonia. What was going on here?



"Success is going from failure to failure without loss of enthusiasm." Winston Churchill
View user's profile View All Posts By User
UnintentionalChaos
International Hazard
*****




Posts: 1454
Registered: 9-12-2006
Location: Mars
Member Is Offline

Mood: Nucleophilic

[*] posted on 9-2-2012 at 11:50


Hydrolysis or formation of biuret. Some is probably unavoidable, keeping the temp lower will help, though recovery will not be as good (hey, urea is dirt cheap anyway) I've had success in using alcohol/water mix to reduce the ridiculous solubility of urea in water, prevention the cooled solution from resembling a brick.

Attachment: ureasolubility.pdf (283kB)
This file has been downloaded 2728 times





Department of Redundancy Department - Now with paperwork!

'In organic synthesis, we call decomposition products "crap", however this is not a IUPAC approved nomenclature.' -Nicodem
View user's profile View All Posts By User
Hexavalent
International Hazard
*****




Posts: 1564
Registered: 29-12-2011
Location: Wales, UK
Member Is Offline

Mood: Pericyclic

[*] posted on 9-2-2012 at 11:52


Thanks!!

I picked up 2kg of urea for 99p at a local discount store, sold for ice removal. As soon as I found its solubility data, I knew it was time to reach for the big flasks:)

Is it possible, out of curiosity, that urea could generate hydrazine on its own?




"Success is going from failure to failure without loss of enthusiasm." Winston Churchill
View user's profile View All Posts By User
Hexavalent
International Hazard
*****




Posts: 1564
Registered: 29-12-2011
Location: Wales, UK
Member Is Offline

Mood: Pericyclic

[*] posted on 9-2-2012 at 11:55


Also, what happens if I accidentally inhale some of the biuret? The MSDS isn't all that helpful. . .



"Success is going from failure to failure without loss of enthusiasm." Winston Churchill
View user's profile View All Posts By User
UnintentionalChaos
International Hazard
*****




Posts: 1454
Registered: 9-12-2006
Location: Mars
Member Is Offline

Mood: Nucleophilic

[*] posted on 9-2-2012 at 11:56


Quote: Originally posted by Hexavalent  
Thanks!!

I picked up 2kg of urea for 99p at a local discount store, sold for ice removal. As soon as I found its solubility data, I knew it was time to reach for the big flasks:)

Is it possible, out of curiosity, that urea could generate hydrazine on its own?


no.

Biuret isn't particularly harmful unless you're a plant. Wikipedia would inform you that it is used as a non-protein nitrogen supplement for animals, if you had bothered to read it.

Also, you see that little button in the top right hand corner of your posts that says "edit?" Use it.

For the multiposts you already made, click edit, check the little box that says "! Delete this message !" and hit edit post.

[Edited on 2-9-12 by UnintentionalChaos]




Department of Redundancy Department - Now with paperwork!

'In organic synthesis, we call decomposition products "crap", however this is not a IUPAC approved nomenclature.' -Nicodem
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 9-2-2012 at 13:12


see last post, this page:

http://www.sciencemadness.org/talk/viewthread.php?tid=7413#p...




The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
Hexavalent
International Hazard
*****




Posts: 1564
Registered: 29-12-2011
Location: Wales, UK
Member Is Offline

Mood: Pericyclic

[*] posted on 9-2-2012 at 14:08


Thankyou UC and Magpie . . .I wasn't aware on how to delete double posts. Like the video on the Grignard reaction BTW UC.



"Success is going from failure to failure without loss of enthusiasm." Winston Churchill
View user's profile View All Posts By User