I decided to start a new experiment a few minutes ago. It involved household products: sodium chloride, acetic acid 8%, hydrogen peroxide and copper.
I was partially influenced by NurdRage's video about cleaning copper coins (loved it).
I wondered about the possibility of making quickly some copper(II) chloride (I had already left some copper wire in the coin-cleaner solution and it
was making copper chloride, but so slow...). I had then the brilliant idea of adding an oxidizer to the old solution, which left my beautiful
blue-green crystals in a bubbling black bud (cupric oxide).
I decided to start a new experiment. I cut some copper wire into a beaker and added 10-volume hydrogen peroxide (yay for household products
experiments!). I added the acetic acid and the salt. It bubbled intensely. The temperature of the beaker wasn't near 100ºC, so I knew it wasn't
boiling. The bluish to green tinge of copper(II) chloride appeared very quickly in the solution.
Gas continued forming. I know some of it is oxygen gas, but the smell wasn't too comfortable. HCl gas would have reacted with copper, so it cannot
possibly be HCl. It didn't have a smell of acetic anhydride. What on earth is it???
This was one of my first equations:
Cu + 2 NaCl + acetic acid ==> CuCl2 + sodium acetate + H2O
What does the H2O2 do to make it so different? Is it the sodium chloride which catalyses the reaction H2O2 ==> H2O+O2?
Please help me.
there may be bugs in gfind
[ˌɛdidʒiˈpiː] IPA pronunciation for my Username
|
|
Hexavalent
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1564
Registered: 29-12-2011
Location: Wales, UK
Member Is Offline
Mood: Pericyclic
|
|
The peroxide helps the copper oxidize to form bivalent aqueous ions.
"Success is going from failure to failure without loss of enthusiasm." Winston Churchill
|
|
Eddygp
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 858
Registered: 31-3-2012
Location: University of York, UK
Member Is Offline
Mood: Organometallic
|
|
But what about the gases. I already know that the copper is a chloride now, but which gases form, apart from the obvious ones?
there may be bugs in gfind
[ˌɛdidʒiˈpiː] IPA pronunciation for my Username
|
|
Hexavalent
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1564
Registered: 29-12-2011
Location: Wales, UK
Member Is Offline
Mood: Pericyclic
|
|
Some would obviously be oxygen, contributed by the decomposition of the peroxide as well.
It could be partially HCl gas, as it wouldn't all necessarily react with the copper. Depending on the temperature of the solution (or maybe not?),
some of it could have been acetic acid vapours, or perhaps even those of some peracetic acid formed.
"Success is going from failure to failure without loss of enthusiasm." Winston Churchill
|
|
kristofvagyok
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 659
Registered: 6-4-2012
Location: Europe
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Eddygp ![](images/xpblue/lastpost.gif) |
Cu + 2 NaCl + acetic acid ==> CuCl2 + sodium acetate + H2O
What does the H2O2 do to make it so different? Is it the sodium chloride which catalyses the reaction H2O2 ==> H2O+O2?
Please help me. |
Copper is only soluble in oxidizing acids, like HNO3, H2SO4, peracetic acid and ect. The H2O2 is needed to make the household vinegar to turn it to
peroxiacetic acid. Also, remember the original producere of copper (II) chloride? HCl and H2O2, it makes active chlorine what will attack the copper.
Normal acetic acid with some table salt won't do anything.
I have a blog where I post my pictures from my work: http://labphoto.tumblr.com/
-Pictures from chemistry, check it out(:
"You can’t become a chemist and expect to live forever."
|
|
Eddygp
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 858
Registered: 31-3-2012
Location: University of York, UK
Member Is Offline
Mood: Organometallic
|
|
It actually did... although maybe it was copper(II) acetate, which would explain the cupric oxide formation.
there may be bugs in gfind
[ˌɛdidʒiˈpiː] IPA pronunciation for my Username
|
|
Eddygp
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 858
Registered: 31-3-2012
Location: University of York, UK
Member Is Offline
Mood: Organometallic
|
|
It is probably acetic acid mist that came out with the oxygen.