Isolating elements with an arc furnace
Hello! I just made a very effective carbon arc furnace. It can easily reach insane temperatures (e.g. I melted a rock into obsidian in under 30
seconds.) Is it possible to isolate elements like silicon from their oxides by placing them with carbon powder and heating them inside the arc? I am
concerned that the element might oxidize again because of the heat.
I made an arc furnace before using a conductive water/sodium bicarbonate mix as a ballast. This new design uses a 1500w space heater as a ballast,
which creates a hotter arc and is safer than the previous method.
[Edited on 5-2-2014 by Gooferking Science]
|
|
bfesser
Resident Wikipedian
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2114
Registered: 29-1-2008
Member Is Offline
Mood: No Mood
|
|
It would be more correct to say that you fused it into a glass, as <a href="https://en.wikipedia.org/wiki/Obsidian"
target="_blank">obsidian</a> <img src="../scipics/_wiki.png" /> is a <em>naturally occurring</em> glass of volcanic origin.
It's bad practice (a bit unscientific) to call any artificially produced materials rocks or minerals.
|
|
Zyklon-A
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1547
Registered: 26-11-2013
Member Is Offline
Mood: Fluorine radical
|
|
What kind of rock was it?
|
|
Gooferking Science
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 97
Registered: 17-7-2013
Location: Somewhere in Kansas, USA...
Member Is Offline
Mood: Halogenated
|
|
It was a lava rock. It "fused" into a glasslike substance similar to obsidian.
bfesser:
If obsidian is of volcanic origin, then can't I have created conditions similar to a volcano? Unless you are meaning that it is artificial obsidian
instead of natural obsidian?
Any comments about the original topic of isolating elements and not rocks?
[Edited on 5-2-2014 by Gooferking Science]
[Edited on 5-2-2014 by Gooferking Science]
[Edited on 5-2-2014 by Gooferking Science]
|
|
Metacelsus
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2534
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline
Mood: Double, double, toil and trouble
|
|
Basically, are you trying to do carbothermal reduction using the arc as a heat source?
According to Wikipedia, "Metallurgical grade silicon is commercially prepared by the reaction of high-purity silica with wood, charcoal, and coal in
an electric arc furnace using carbon electrodes."
So isolating silicon has a good chance of success.
From my personal experience with arcs, I recommend using an inductive ballast (you can easily make one from a microwave oven transformer core). They
don't heat up as much.
|
|
thebean
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 116
Registered: 26-9-2013
Location: Minnesota
Member Is Offline
Mood: Deprotonated
|
|
Even if the conditions are similar to that of a volcano, it didn't come from a volcano. It would also be incorrect to call it artificial obsidian
because the one of the conditions for something to be called obsidian is that it occurs naturally. You made a glass of some kind.
"You need a little bit of insanity to do great things."
-Henry Rollins
|
|
chemrox
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline
Mood: LaGrangian
|
|
Would you like to outline the oven construction? That would be a worthwhile contribution.
Artificial diamonds are still referred to as "diamonds." If you took rhyolite and changed its texture by fusing it with heat you may have made
"obsidian." I'd have to see it. On the other hand maybe what you made is more properly referred to as "slag." Got a picture of the resultant?
"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
|
|