Mickhael
Hazard to Self

Posts: 65
Registered: 17-11-2004
Location: B.C. Canada
Member Is Offline
Mood: Terrificlawful
|
|
Making a compression controled Hydraulic Press?
I'm wondering if anyone has plans for building a compress at home, I know small 2 ton presses are easily bought at auto shops for $20 or so,
could this be mounted upside down, and the compression rate controlled by an electric tire pump or something? In order to compress different materials
at certain pressures. Such as for making quality black powder, I've read a compress is needed, although the plans I found are not controllable
like I would prefer. Any idea's or plans? I'm hoping to build one this year. Thankyou.
|
|
|
cyclonite4
Hazard to Others
 
Posts: 480
Registered: 16-11-2004
Location: is unknown
Member Is Offline
Mood: Amphoteric
|
|
Here is a plan I stumbled upon while I while i was at E&W: http://www.wecreate4u.net/dwilliams/press/press.html
This one is fairly basic, but the author speaks somewhere on his website about an electrically controlled press that can put fairly large pressures at
the press of a button.
\"It is dangerous to be right, when your government is wrong.\" - Voltaire
|
|
|
Mickhael
Hazard to Self

Posts: 65
Registered: 17-11-2004
Location: B.C. Canada
Member Is Offline
Mood: Terrificlawful
|
|
Ah thankyou, I have heard of that site before, but the refresher look gave me some idea's...so thankyou indeed, and I will look further into
using the torque wrench for compression control
|
|
|
cyclonite4
Hazard to Others
 
Posts: 480
Registered: 16-11-2004
Location: is unknown
Member Is Offline
Mood: Amphoteric
|
|
I'm thinking of building one myself and was just wondering (I'm no auto expert ) whether or not hydraulic jacks are expensive...
I saw one at a garage sale for a few dollars, but I didnt buy it considering the jack was rusted all over.
\"It is dangerous to be right, when your government is wrong.\" - Voltaire
|
|
|
Mickhael
Hazard to Self

Posts: 65
Registered: 17-11-2004
Location: B.C. Canada
Member Is Offline
Mood: Terrificlawful
|
|
To my knowledge they are dirt cheap, down at several local auto shops, I can buy a 2 ton, with a 1" head for $20 cdn...you should have no problem
getting the same, they are mostly used for jacking small vehicles up to change a tire.
|
|
|
Mr. Wizard
International Hazard
   
Posts: 1042
Registered: 30-3-2003
Member Is Offline
Mood: No Mood
|
|
Don't buy the 2 ton automotive jacks, for a few dollars more you can get a 12 ton one . Go to your local "Harbor Freight Tools", or
you local equivalent, and you can get a much heavier one. You can buy a pre-made press with the jack included "Central Hydraulics" brand for
$99. I'm trying to figure out if I can put a gauge on the cylinder pressure to figure the actual pressure.
|
|
|
cyclonite4
Hazard to Others
 
Posts: 480
Registered: 16-11-2004
Location: is unknown
Member Is Offline
Mood: Amphoteric
|
|
12 ton... NICE 
Even though they can be bought, I would prefer making it, because I enjoy such projects.
EDIT: BTW, I was referring to the pre-made press.
[Edited on 18-1-2005 by cyclonite4]
\"It is dangerous to be right, when your government is wrong.\" - Voltaire
|
|
|
Mickhael
Hazard to Self

Posts: 65
Registered: 17-11-2004
Location: B.C. Canada
Member Is Offline
Mood: Terrificlawful
|
|
Ya I'm totally doing this as well because I like making my own things, and it makes for more learning and can sometimes be cheaper as well (as
long as you don't count the man hours) lol...
Also I don't see the point of buying a 12 ton press...when your only going to use between 2lb and 500lb for most uses....unless your also using
it for thick metal pressing....that kind of power is way overkill.
(sorry, meant 500lb not 50lb)
[Edited on 19-1-2005 by Mickhael]
\"I shall not fear, fear is the mind killer...\"
|
|
|
Mr. Wizard
International Hazard
   
Posts: 1042
Registered: 30-3-2003
Member Is Offline
Mood: No Mood
|
|
I won't bother with all the uses of a 12 ton press, but if you only need 2 to 50 pounds don't waste your money, just lean on it. As to DIY ,
making the whole thing does have it's appeal. I have all the tools to make one, but I haven't done it yet, and I'm still deciding if
the $60 extra for the whole press is worth the extra cost of driving around and buying, then designing, cutting, drilling, and painting the metal to
make it. Never mind, I just decided.
|
|
|
solo
International Hazard
   
Posts: 3975
Registered: 9-12-2002
Location: Estados Unidos de La Republica Mexicana
Member Is Offline
Mood: ....getting old and drowning in a sea of knowledge
|
|
Ref: Pill Press
Here is a link to a forum where someone else is trying to do the same thing......solo
http://www.wetdreams.ws/forum/topic.asp?TOPIC_ID=1979
It's better to die on your feet, than live on your knees....Emiliano Zapata.
|
|
|
cyclonite4
Hazard to Others
 
Posts: 480
Registered: 16-11-2004
Location: is unknown
Member Is Offline
Mood: Amphoteric
|
|
I'm gonna build it myself not only for the fun, but because I trust and like my creations better than the commerical versions.
\"It is dangerous to be right, when your government is wrong.\" - Voltaire
|
|
|
Mickhael
Hazard to Self

Posts: 65
Registered: 17-11-2004
Location: B.C. Canada
Member Is Offline
Mood: Terrificlawful
|
|
Ok...just to clarify...
Wizard...I appreciate the thoughts, and I agree that for the trouble, if your not into building your own, buying is the solution. However not only do
I want an adjustable press, I do not want to be "leaning over/on" what I am pressing...I want to be a damn good distance away...if you catch
my drift. And the ability to exactly control the compression is quite important to my mind...and overkill is not a good thing, but neither is to
little...hence the "low, controled compression".
\"I shall not fear, fear is the mind killer...\"
|
|
|
trilobite
Hazard to Others
 
Posts: 152
Registered: 25-2-2004
Location: The Palaeozoic Ocean
Member Is Offline
Mood: lonely
|
|
Auto-stop hydraulic press
These guys use a hydraulic press with an adjustable torque wrench, all something you can get at a hardware store. I think the PDF is missing an image
of the actual press, I can scan the hardcopy version if needed.
A Low-Cost Auto-Stop Hydraulic Press for Making KBr Disc
Journal of Chemical Education 75, 629 (1998)
Attachment: J_Chem_Educ_75_629.pdf (85kB) This file has been downloaded 957 times
|
|
|